Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 45 - 60 min | 45 - 60 min | Mass: 100g; TM R050-17 |
Resinlab® EP1285HD-9 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |
|||
Pot Life | 45 min | 45 min | |
NextGen Adhesives M907-11 Medical Grade Epoxy Adhesive Description: NGAC M907-11 is a medium viscosity adhesive system that is specifically formulated for medical device assembly applications.Advantages and Applications: Uses include laminating, bonding.. |
|||
Pot Life | 45 min @Temperature 25.0 °C |
45 min @Temperature 77.0 °F |
|
Parker Chomerics Tecknit® 72-00008 Silver-Filled Epoxy System Description: This commercial grade, conductive epoxy is designed for use in bonding applications where good conductivity is required. When mixed in a ratio of 1:1.4 by volume or weight, the two comp.. |
|||
Pot Life | 45 min @Temperature 25.0 °C |
45 min @Temperature 77.0 °F |
|
Parker Chomerics Tecknit® 72-08116 Silver-Filled Epoxy System Description: This is a silver filled epoxy system designed for maximum performance and lowest volume resistivity. It is easily mixed 1:1 by volume or weight, from the two one-ounce jars. Its consist.. |
|||
Pot Life | 45 min | 45 min | Ambient |
Reltek BONDiT™ B-536 Adhesive System Key Properties: Very high strength bonding of dissimilar materials.High moisture and solvent resistance.Fast ambient cure with good pot life.Ease of use.Applications: Outstanding adhesive for very h.. |
|||
Pot Life | 45 min | 45 min | Mass: 100g; TM R050-19 |
Resinlab® EP1385 Black Epoxy Formulation Resinlab™ EP1385 Black is an epoxy formulation designed for applications requiring resistance to E-85 type fuels. It has good wetting and adhesion to most surfaces. It has very good resistance to w.. |
|||
Pot Life | 45 min | 45 min | Mass: 200g; TM R050-19 |
Resinlab® EP1390 Medium Viscosity, Self Extinguishing Flame Retardant Epoxy Casting Resin System Resinlab™ EP1390 is a RoHS compliant, medium viscosity, self extinguishing flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Labor.. |
|||
Pot Life | >= 45 min | >= 45 min | |
Abatron 2217 A/B Filled Potting Compound
(discontinued **) Gray versatile potting casting adhesive resurfacing compound. 2/1 variable ratio.Information provided by Abatron. |
|||
Pot Life | >= 45 min | >= 45 min | |
Abatron 416 A/B Filled Potting Compound
(discontinued **) Phosphorescent litegreen resin. 100/26 ratio.Information provided by Abatron. |
|||
Pot Life | >= 45 min | >= 45 min | |
Abatron 85083 A/B Filled Potting Compound
(discontinued **) Standard versatile, good color retention. 100/20 ratio.Information provided by Abatron. |
|||
Pot Life | 45 - 60 min | 45 - 60 min | |
Aremco Aremco-Bond™ 597 Conductive Epoxy Adhesive
(discontinued **) Electrically and thermally conductive, silver-filled, one-part paste. Inorganic system for adhesive (597A) & coating (597C) applications to 1200 ºF (650 °C). |
|||
Pot Life | 45 min | 45 min | |
Huntsman HY 2963 Cycloaliphatic Amine Approx. H+ equivalent weight 85. Mix Ratio with GY 6010 is 45.Comments/Applications: Phenol-free version of HY 2964. Mortar and floor repair, sewage treatment plants, commercial and industrial fl.. |
|||
Pot Life | 45 - 75 min | 45 - 75 min | 100 gram batch |
Master Bond EP42HT-2Med Epoxy Meets USP Class VI Requirements Description: Master Bond Polymer System EP42HT-2Med is a room temperature curable two component epoxy, adhesive, sealant, coating and casting material featuring high temperature resistance along wit.. |
|||
Pot Life | 45 - 60 min | 45 - 60 min | 100 gm mass |
Master Bond EP79 Two Component, Silver Coated, Nickel Filled Conductive Epoxy Master Bond Polymer System EP79 is a two component, silver coated, nickel filled, electrically conductive adhesive for high performance bonding and sealing formulated to cure at room temperature or .. |
|||
Pot Life | 45 min | 45 min | 25 grams |
Tra-Con Tra-Bond 2119 Low Viscosity Glass Laminating Adhesive TRA-BOND 2119 is a crystal clear adhesive specifically designed for bonding glass to glass and glass to plastics. It also yields a high lap shear strength to metals and ceramics. This system cures t.. |
|||
Pot Life | 45 min | 45 min | |
Tra-Con Tra-Bond FDA2 Food and Drug Application Epoxy Adhesive TRA-BOND FDA-2 is a medium viscosity epoxy resin system specifically developed for medical device applications. It has been tested in accordance with USP biological reactivity tests, in vivo and rec.. |
|||
Pot Life | 45 min | 45 min | |
Tra-Con Tra-Bond FS482 Long Pot Life High Tg Fiber Optic Epoxy Adhesive TRA-BOND FS-482 is a dark blue, low viscosity epoxy adhesive developed for fiber-optic bonding and small volume potting of plastic or glass optical fibers, lenses and prisms, LED displays, and other.. |
|||
Pot Life | 45 - 75 min | 45 - 75 min | 100 gram batch |
Master Bond EP42HT-2FG Two Component Epoxy Adhesive for Food Applications Master Bond Polymer System EP42HT-2FG is a room temperature setting, two component epoxy adhesive, sealant and coating specially formulated for food applications. It has been independently tested an.. |
|||
Pot Life | 45 min | 45 min | |
Abatron AboCoat 8709-8/AboCure 50-12 Nickel-Filled Electrically Conductive Epoxy Compound AboCoat 8709-8/AboCure 50-12 is a versatile nickel-epoxy conductive coating. |
|||
Pot Life | <= 45 min | <= 45 min | |
Abatron AboTar 8607-1 Solventless Tar-Epoxy Compound AboTar 8607-1 is a 2-part tar-epoxy lower cost system for filling and leveling pot holes and grossly uneven flooring. It can be used neat or with sand or aggregates. Uses: Resurfacing concrete and .. |
|||
Pot Life | 45 min @Temperature 24.0 °C |
45 min @Temperature 75.2 °F |
1 lb. mass |
BCC Products BC 6126 Epoxy Surface Coat/Casting BC 6126 is a gray, low toxicity, aluminum filled, epoxy surface coat. This thixotropic resin system provides excellent surface duplication along with vertical coverage to 1/16 inch thickness. This h.. |
|||
Pot Life | 45 - 60 min | 45 - 60 min | Mass: 50g; TM R050-19 |
Resinlab® EP965SC-7 Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965SC-7 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wett.. |
|||
Pot Life | 45 min | 45 min | Mass: 5g; TM R050-19 |
Resinlab® SEC1222 Silver Filled Epoxy Adhesive Resinlab™ SEC1222 is a silver filled, two component, room temperature curing epoxy adhesive. It is designed to cure completely at room temperature. SEC1222 provides excellent electrical conductivit.. |
|||
Pot Life | 45 - 75 min | 45 - 75 min | 100 gram mass |
Master Bond EP39MHT Two Component, Room Temperature Curing Epoxy Resin System Master Bond Polymer System EP39MHT is a low viscosity, two component, epoxy resin system for high performance potting, encapsulation, sealing and bonding. It cures readily at ambient temperatures to.. |