Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 3.00 min | 3.00 min | |
Northstar Polymers MSB-A95A High Performance Polyurethane Cast Elastomer System This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires high tensile strength, cut/tear resistance, dry-abrasio.. |
|||
Pot Life | 3.00 min | 3.00 min | |
Northstar Polymers MSS-A70GQ High Performance Polyurethane Cast Elastomer System 70A This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires cut/tear resistance, dry-abrasion resistance, slow resp.. |
|||
Pot Life | 3.00 - 4.00 min @Temperature 20.0 °C |
3.00 - 4.00 min @Temperature 68.0 °F |
|
Permabond ET500 Epoxy Resin PERMABOND ET500 is a two-part fast-setting epoxy adhesive which bonds to a wide variety of substrates such as wood, metal, ceramics and some plastics and composites. It cures rapidly at room tempera.. |
|||
Pot Life | 3.00 min @Temperature 23.9 °C |
3.00 min @Temperature 75.0 °F |
|
3M Scotch-Weld™ 3535 B/A Off-white Two-Part Urethane Adhesive 3535 B/A Off-white
(discontinued **) Two-part urethane adhesives cure at room temperature or with heat to provide tough, impact resistant bonds with high peel strength. Features include fast cure adhesive, 15-20 minutes handling stren.. |
|||
Pot Life | 3.00 min | 3.00 min | |
Northstar Polymers MPG-D70A Room-Temperature-Curable Polyurethane Casting Elastomer MPG-D70A is room-temperature-curable polyurethane casting elastomer system designed for molding polyurethane parts with tough, but flexible physical characteristics. The typical applications for th.. |
|||
Pot Life | 3.00 min @Temperature 23.9 °C |
3.00 min @Temperature 75.0 °F |
|
ITW Devcon Rubber Repair / Castable Urethane High Temp Edge & Seal (T-36), Amber Information provided by ITW Devcon |
|||
Pot Life | 3.00 min @Temperature 23.9 °C |
3.00 min @Temperature 75.0 °F |
|
ITW Devcon Rubber Repair / Castable Urethane Edge & Seal (T-35), Black Information provided by ITW Devcon |
|||
Pot Life | 3.00 min | 3.00 min | uncured |
Atom Adhesives AA-BOND 201 Epoxy Adhesive AA-BOND 201 is an exceptional epoxy formulation recommended for lower temperature or wet industrial bonding applications where FAST CURING is required. AA-BOND 201 is versatile two-part epoxy system.. |