Processing Properties | Metric | English | Comments |
---|---|---|---|
Head Temperature | 190 - 200 °C | 374 - 392 °F | Average value: 195 °C Grade Count:4 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a.. |
|||
Head Temperature | 190 - 200 °C | 374 - 392 °F | Extrusion Molding |
Kolon ELLAS K-385A Ether Based Thermoplastic Polyurethane ApplicationsExtrusionInjection: Cable Sheathing, High pressure tubeWheelCaster Information provided by API-Kolon. |
|||
Head Temperature | 190 - 200 °C | 374 - 392 °F | Extrusion Molding |
Kolon ELLAS K-390A Ether Based Thermoplastic Polyurethane ApplicationsExtrusion: Cable Sheathing, high pressure tubeInjectionElectric WireIndustry Parts Information provided by API-Kolon. |
|||
Head Temperature | 190 - 200 °C | 374 - 392 °F | Extrusion Molding |
Kolon ELLAS K-395A Ether Based Thermoplastic Polyurethane ApplicationsExtrusionInjection: Cable sheathing, Highly Pressurized HoseIndustry Parts Information provided by API-Kolon. |
|||
Head Temperature | 190 - 200 °C | 374 - 392 °F | Extrusion Molding |
Kolon ELLAS K-395F Ether Based Thermoplastic Polyurethane ApplicationsExtrusionHighly Pressurized Hose Information provided by API-Kolon. |
|||
Head Temperature | 190 - 205 °C | 374 - 401 °F | Extrusion Molding |
Kolon ELLAS K-429A Ester Based Thermoplastic Polyurethane ApplicationsIndustry PartsOutsole of Soccer ShoeHighly Pressurized Hose Information provided by API-Kolon. |
|||
Head Temperature | 190 - 200 °C | 374 - 392 °F | Extrusion Molding |
Kolon ELLAS K-470A Ester Based Thermoplastic Polyurethane ApplicationsInjectionIndustry PartsParts for Automobile/Mobile phoneABS Compound |
|||
Head Temperature | 190 - 200 °C | 374 - 392 °F | Extrusion Molding |
Kolon ELLAS K-480A Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionCompoundingIndustry PartsParts for Automobile/Mobile phoneAcetal Compound Information provided by API-Kolon. |
|||
Head Temperature | 190 - 205 °C | 374 - 401 °F | Extrusion Molding |
Kolon ELLAS K-490AB Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionFilm/SeatBlown filmIndustry Parts Information provided by API-Kolon. |
|||
Head Temperature | 190 - 200 °C | 374 - 392 °F | Extrusion Molding |
Kolon ELLAS K-585A Caprolactone Based Thermoplastic Polyurethane ApplicationsInjectionIndustry Parts Information provided by API-Kolon. |
|||
Head Temperature | 190 - 200 °C | 374 - 392 °F | Extrusion Molding |
Kolon ELLAS K-590A Caprolactone Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionDust SealOil Seal Information provided by API-Kolon. |
|||
Head Temperature | 190 - 200 °C | 374 - 392 °F | Extrusion Molding |
Kolon ELLAS K-596A Caprolactone Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionDust SealOil Seal Information provided by API-Kolon. |
|||
Head Temperature | 190 - 200 °C | 374 - 392 °F | Extrusion Molding |
Kolon ELLAS K-787A Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionFlexible HoseIndustry Parts Information provided by API-Kolon. |
|||
Head Temperature | 190 °C | 374 °F | |
Lotte Chemical Titan TITANEX® HB0972 High density polyethylene Hexene-1 resin HF0972 is a pelleted high density polyethylene Hexene-1 resin for blow molding.Applications: Large size shipping containers and drums, household and industrial chemical containers, toiletries and c.. |
|||
Head Temperature | 190 - 210 °C | 374 - 410 °F | |
Borealis Borcoat™ HE3450 Black High Density Polyethylene Top Coat for Steel Pipe Coating Borcoat HE3450 is a black, high-density polyethylene (HDPE) produced with the advanced Borstar technology, providing the material with especially well melt strength and extrudability. Also its mech.. |
|||
Head Temperature | 190 - 210 °C | 374 - 410 °F | |
Borealis Borcoat™ HE3453 Natural High Density Polyethylene for Steel Pipe Coating Borcoat HE3453 is a natural and colorable high density polyethylene produced with the Borstar technology in similar conditions as the black ready made top coat Borcoat HE3450. Borcoat HE3453 is rec.. |
|||
Head Temperature | 190 °C | 374 °F | die head |
Borealis Borstar® LE8706 Natural Bimodal LLDPE Jacketing Compound for Energy and Communication Cables Borstar® LE8706 is a natural colorable linear low density (LLD) jacketing compound, which is produced with the Borealis proprietary Borstar® bimodal process technology. Borstar technology allows .. |
|||
Head Temperature | >= 190 °C | >= 374 °F | |
Borealis Casico™ FR4805 Non Halogen Flame Retardant Compound for Sheathing Energy Cables Casico FR4805 is a thermoplastic, non-halogen containing natural jacketing compound. It combines high mechanical strength and toughness with flame retardancy. The composition of Casico FR4805 is b.. |
|||
Head Temperature | 190 °C | 374 °F | |
Borealis LE0574 Polyethylene LE0574 is a thermoplastic black polyethylene compound, specially designed for strippable semi conductive screen applications. It can be used in thermoplastic form or crosslinked via a grafting proce.. |
|||
Head Temperature | >= 190 °C | >= 374 °F | |
Borealis Visico™ ME4425/LE4462 Scorch Retardant Silane Crosslinkable MDPE Track Resistant Cable Insulation Visico ME4425/LE4462 is a combination of LE4425, a Medium Density Visico base resin and a masterbatch, LE4462, which contains catalyst, carbon black, UV stabilizers and antioxidants. The LE4462 mas.. |
|||
Head Temperature | >= 190 °C | >= 374 °F | |
Borealis Casico™ FR4802 Non-Halogen Flame Retardant Insulation/Jacketing Compound Borstar FR4802 is a natural, thermoplastic polyolefin compound designed for flame retardant low voltage wire insulation and jacketing. As such, FR4802 offers a unique combination of good extrusion p.. |
|||
Head Temperature | 190 °C | 374 °F | die head |
Borealis Borstar® LE8707 Black Bimodal LLDPE Jacketing Compound for Energy and Communication Cables Borstar® LE8707 is a black linear low density (LLD) jacketing compound, which is produced with the Borealis proprietary Borstar® bimodal process technology. Borstar® technology allows the manufa.. |