Processing Properties Metric English Comments
Head Temperature 130 - 150 °C
266 - 302 °F
Fainplast Compounds HAX HFX 024-15C Halogen Free PVC
This product is a LSFOH silane grafted compound for cable insulation and sheating, cross-linkable by heat and moisture by previous addition of a suitable catalyst masterbatch. It is recommended to s..
Head Temperature 130 - 150 °C
266 - 302 °F
Fainplast Compounds HAX HFX 024-21L Halogen Free PVC
This product is a LSFOH silane grafted compound for cable insulation and sheating, cross-linking by heat and moisture by previous addition of a suitable catalyst masterbatch. It is highly recommende..
Head Temperature 130 - 165 °C
266 - 329 °F
Average value: 146 °C Grade Count:3
Overview of materials for PVC, Wire and Cable Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Wire and Cable Grade". Each property range of values reported is minimum and maximum values of appr..