Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem 8075 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem AB760LG TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem AB845EM TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem AB860EM TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem AB870EM TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem AB870LG TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem DIOSHY® GP-935-UB2 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem DIOSHY® MP-960NC TPE Compound This grade of Stellarchem MP series is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, styrene block copolymers based, .. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem GP-785A TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem GP-860 TPE Compound Product description : This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric poly.. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem GP-860HD TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem GP-930 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem GP-9401 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem GP-945 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem GP-950 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem GP-965B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem GP-975 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem LP-870 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem LP-880 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem MP-835B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem MP-930HD TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem MP-950NC TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem SV-B70E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem SV-B75E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem 475-845N TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Injection Pressure | 5.00 - 40.0 MPa | 725 - 5800 psi | Injection Molding |
Stellarchem MP-855WR TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Injection Pressure | 30.0 - 40.0 MPa | 4350 - 5800 psi | |
Toyobo GLAMIDE® T-662 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Injection Pressure | 30.0 - 40.0 MPa | 4350 - 5800 psi | (DAM) |
Toyobo T-661 Nylon 66, Standard Grade (Conditioned) Features: Non-reinforced, Standard GradeInformation provided by Toyobo. |
|||
Injection Pressure | 30.0 - 40.0 MPa | 4350 - 5800 psi | |
Toyobo GLAMIDE® T-802 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Injection Pressure | 30.0 - 40.0 MPa | 4350 - 5800 psi | |
Toyobo T-661 Nylon 66, Standard Grade (DAM) Features: Non-reinforced, Standard GradeInformation provided by Toyobo. |