Injection Pressure |
90.0 - 110 MPa |
13100 - 16000 psi |
|
Polykemi AB POLYelast TPE R44 Thermoplastic Elastomer
Information provided by Polykemi AB |
Injection Pressure |
40.0 - 110 MPa |
5800 - 16000 psi |
|
Polykemi AB POLYfill PP CIQ10015ER UV Polypropylene, Mineral Reinforced
Information provided by Polykemi AB |
Injection Pressure |
40.0 - 110 MPa |
5800 - 16000 psi |
|
Polykemi AB POLYfill PP HIP16020FCF Polypropylene, Fast Cycle
Information provided by Polykemi AB |
Injection Pressure |
40.0 - 110 MPa |
5800 - 16000 psi |
|
Polykemi AB POLYfill PPC GF2007 PD1 Polypropylene Copolymer, Glass Fiber Reinforced, Chemically Coupled
Information provided by Polykemi AB |
Injection Pressure |
40.0 - 110 MPa |
5800 - 16000 psi |
|
Polykemi AB POLYfill PPC K20010 PP, 10% Mineral Reinforced
Information provided by Polykemi AB |
Injection Pressure |
40.0 - 110 MPa |
5800 - 16000 psi |
|
Polykemi AB POLYfill PPC K20040 Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB |
Injection Pressure |
40.0 - 110 MPa |
5800 - 16000 psi |
|
Polykemi AB POLYfill PPC T1030 Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB |
Injection Pressure |
40.0 - 110 MPa |
5800 - 16000 psi |
|
Polykemi AB POLYfill PPC T4020 H Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB |
Injection Pressure |
40.0 - 110 MPa |
5800 - 16000 psi |
|
Polykemi AB POLYfill PPH GF5020 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled
Information provided by Polykemi AB |
Injection Pressure |
40.0 - 110 MPa |
5800 - 16000 psi |
|
Polykemi AB POLYfill PPH GK8020D Polypropylene Homopolymer, Glass Reinforced, Detergent Resistant
Information provided by Polykemi AB |
Injection Pressure |
40.0 - 110 MPa |
5800 - 16000 psi |
|
Polykemi AB POLYfill PPH GK8040 Polypropylene Homopolymer, Glass Reinforced
Information provided by Polykemi AB |
Injection Pressure |
40.0 - 110 MPa |
5800 - 16000 psi |
|
Polykemi AB POLYfill PPH T15040 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB |
Injection Pressure |
40.0 - 110 MPa |
5800 - 16000 psi |
|
Polykemi AB POLYfill PP TOUCH 25325 R3 Polypropylene, Glass Fiber Reinforced, Scratch Resistant
Information provided by Polykemi AB |
Injection Pressure |
40.0 - 110 MPa |
5800 - 16000 psi |
|
Polykemi AB POLYfill PPC BGK601213 CR Polypropylene Copolymer, Multifiller
Information provided by Polykemi AB |
Injection Pressure |
40.0 - 110 MPa |
5800 - 16000 psi |
|
Polykemi AB POLYfill PPH B8065 VT1 Polypropylene Homopolymer, Mineral Reinforced, Heat Resistant
Information provided by Polykemi AB |
Injection Pressure |
40.0 - 110 MPa |
5800 - 16000 psi |
|
Polykemi AB POLYfill PPH GF35040 D PP, Glass Fiber-Reinforced, Chemically Coupled, Detergent Resistant
Information provided by Polykemi AB |
Injection Pressure |
40.0 - 110 MPa |
5800 - 16000 psi |
|
Polykemi AB POLYfill PPH GF5030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled
Information provided by Polykemi AB |
Injection Pressure |
40.0 - 110 MPa |
5800 - 16000 psi |
|
Polykemi AB POLYfill PPH MGF5040 Polypropylene Homopolymer, Multifiller
Information provided by Polykemi AB |
Injection Pressure |
40.0 - 110 MPa |
5800 - 16000 psi |
|
Polykemi AB POLYfill PPH Q15030 E10 Polypropylene Homopolymer, Mineral Reinforced, Elastomer Modified
Information provided by Polykemi AB |
Injection Pressure |
40.0 - 110 MPa |
5800 - 16000 psi |
|
Polykemi AB POLYfill PPH T10020 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB |
Injection Pressure |
40.0 - 110 MPa |
5800 - 16000 psi |
|
Polykemi AB POLYfill PPC GF5020 Polypropylene Copolymer, Glass Fiber Reinforced
Information provided by Polykemi AB |
Injection Pressure |
40.0 - 110 MPa |
5800 - 16000 psi |
|
Polykemi AB POLYfill PPC T5020 Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB |
Injection Pressure |
40.0 - 110 MPa |
5800 - 16000 psi |
|
Polykemi AB POLYfill PPH T5060 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB |
Injection Pressure |
40.0 - 110 MPa |
5800 - 16000 psi |
|
Polykemi AB POLYfill PPH TS8038 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB |
Injection Pressure |
40.0 - 110 MPa |
5800 - 16000 psi |
|
Polykemi AB POLYfill PPHC K8040G E10 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB |
Injection Pressure |
40.0 - 110 MPa |
5800 - 16000 psi |
|
Polykemi AB POLYfill PPH TS2040 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB |