Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Injection Pressure 6.21 - 12.4 MPa
900 - 1800 psi
Ravago Manufacturing Americas Hylex® P1018LLT Polycarbonate
Information provided by Ravago.
Injection Pressure 6.21 - 12.4 MPa
900 - 1800 psi
Ravago Manufacturing Americas Hylex® P1318LLT Polycarbonate
Information provided by Ravago.
Injection Pressure 6.21 - 12.4 MPa
900 - 1800 psi
Entec Hylex® P1017FR Polycarbonate
Information provided by Ravago.
Injection Pressure 6.21 - 12.4 MPa
900 - 1800 psi
Entec Hylex® P1317FR Polycarbonate
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..