Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 60.0 - 70.0 MPa | 8700 - 10200 psi | |
Plastcom PLASTALEN® PH 91 SD Polypropylene Modified homopolymer PP for injection molding. General use in all industry branches. Delivered in natural mode and in the full RAL color scale.Information Provided by Plastcom spol. s r.o. |
|||
Injection Pressure | 60.0 - 100 MPa | 8700 - 14500 psi | |
Plastcom SLOVASTER® B GF 6 FRL 4 PBT, 6% glass fibre, flame retarder FeaturesPBT with the content of 6 % chemically bound glass fibre and with the flame retardant on the basis of bromine hydrocarbons. Anisotropy of shrinkage enables the injection moulding of round, c.. |
|||
Injection Pressure | 60.0 - 100 MPa | 8700 - 14500 psi | |
SABIC MG200024 Linear Low Density Polyethylene for Compounding Product Description: MG200024 is a Linear Low Density Polyethylene grade with a narrow molecular weight distribution primarily suitable for compounding. It is in the powder form designed to give g.. |
|||
Injection Pressure | 60.0 - 80.0 MPa | 8700 - 11600 psi | |
Premix Thermoplastics PRE-ELEC® PE 1296 Conductive Thermoplastic Compound PRE-ELEC® PE 1296 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1296 has a high concentration o.. |
|||
Injection Pressure | 60.0 MPa | 8700 psi | |
Ineos ABS Centrex® 814 ASA Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingInformation provided by Ba.. |
|||
Injection Pressure | 60.0 MPa | 8700 psi | |
Covestro Makroblend® UT-250 Polycarbonate + Polyester Blend Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015,.. |
|||
Injection Pressure | 60.0 MPa | 8700 psi | |
Covestro Makroblend® UT-640 G Polycarbonate + Polyester Blend Key Features:Contains FillerHigh impact or high impact modifiedLight stabilized or stable to lightSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 Septembe.. |
|||
Injection Pressure | 60.0 - 70.0 MPa | 8700 - 10200 psi | |
Plastcom SLOVALEN PH 91 N Polypropylene Homopolymer FeaturesModified homopolymer PP for injection moulding. General use in all industry branches - packing material, garden flower-pots, toys, furniture industry, hinges, fasteners, clamps, office chai.. |
|||
Injection Pressure | 60.0 - 100 MPa | 8700 - 14500 psi | |
Plastcom SLOVASTER® B2 BT PBT, basic type FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of.. |
|||
Injection Pressure | 60.0 - 80.0 MPa | 8700 - 11600 psi | |
Premix Thermoplastics PRE-ELEC® PA 1411 Conductive Thermoplastic Compound PRE-ELEC® PA 1411 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. PRE-ELEC® PA 1411 has a very low electrical resistivity. P.. |
|||
Injection Pressure | 60.0 - 80.0 MPa | 8700 - 11600 psi | |
Premix Thermoplastics PRE-ELEC® ESD 12-000
(discontinued **) PRE-ELEC ESD 12-000 is a static dissipative thermoplastic compound based on polyacetal copolymer. The dissipative property is permanent and built into the polymer chain. The products made out of PRE.. |
|||
Injection Pressure | 60.0 - 80.0 MPa | 8700 - 11600 psi | Average value: 70.0 MPa Grade Count:4 |
Overview of materials for Polypropylene with Carbon Black Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v.. |