Polymer Property : Ejection Temperature = 248 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Ejection Temperature 120 °C
248 °F
Covestro Bayblend® KU 2-1446 Polycarbonate + ABS Blend  (discontinued **)
Key Features:UnfilledPlatableSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bay..
Ejection Temperature 120 °C
248 °F
Covestro Bayblend® FR 3030 Polycarbonate + ABS, Flame Retardant Grade
Flame retardant extrusion gradeVicat/B 120 temperature = 115 °Cgood extrusion and vacuum-forming behaviourUL-listing 94 V-0 (1.5 mm)halogen-free according to DIN VDE 0472-815glow wire temperature (..
Ejection Temperature 120 °C
248 °F
Covestro Bayblend® T65 Polycarbonate + ABS
General purpose injection molding gradeVicat/B 120 temperature = 120 °Cgood low temperature impact strengthPreprocessingMax. Water content
Ejection Temperature 120 °C
248 °F
Covestro Bayblend® T65 XF Polycarbonate + ABS
General purpose injection molding gradeVicat/B 120 temperature = 120 °Cimproved flowability compared to T65PreprocessingMax. Water content
Ejection Temperature 120 °C
248 °F
Covestro Bayblend® KU 1-1446* Polycarbonate + ABS
Developmental productGrade with improved low-temperature impact strength and petrol resistance for automotive partsin version BBS904 suitable for extrusion/extrusion blow molding and electroplating ..