Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 190 - 265 °C | 374 - 509 °F | Cylinder temp |
Techno Polymer Techno ABS LM100 Transparent Excellent shock resistance, rigidity, and processability.Applications: Appliance parts, office and computer equipment, machine parts, and tool handles. |
|||
Processing Temperature | 190 - 265 °C | 374 - 509 °F | Average value: 223 °C Grade Count:5 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m.. |
|||
Processing Temperature | 190 - 265 °C | 374 - 509 °F | Cylinder temp |
Techno Polymer Techno ABS LM100 Transparent Excellent shock resistance, rigidity, and processability.Applications: Appliance parts, office and computer equipment, machine parts, and tool handles. |
|||
Processing Temperature | 255 - 265 °C | 491 - 509 °F | |
Zhejiang Juner 201-G20 20% Glass Fibre Reinforced Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Processing Temperature | 255 - 265 °C | 491 - 509 °F | |
Zhejiang Juner 201-G30 30% Glass Fibre Reinforced Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Processing Temperature | 215 - 265 °C | 419 - 509 °F | |
E-Polymers Tekaloy® G70NH Non-Halogen Flame Retardant, Un-Reinforced PC/ABS Alloy Non Halogen Flame Retardant, High FlowInformation provided by E-Polymers Co. Ltd. |
|||
Processing Temperature | 70.0 - 265 °C | 158 - 509 °F | Average value: 198 °C Grade Count:43 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi.. |