Polymer Property : Processing Temperature = 419 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 215 - 232 °C
419 - 450 °F
Preheat
Solvay Specialty Polymers Hylar® 460 PVDF Polyvinylidene Fluoride  (discontinued **)
Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a..
Processing Temperature 215 - 232 °C
419 - 450 °F
Preheat
Solvay Specialty Polymers Hylar® MP10 PVDF Polyvinylidene Fluoride  (discontinued **)
Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a..
Processing Temperature 215 °C
419 °F
Die temperature
EVALCA EVAL® EP-J102B Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
32 mol % Ethylene.Data provided by EVALCA. Designed to provide a wide thermoforming range together with high barrier properties. EVAL® EP-J102B is specifically designed for thermoforming applicat..
Processing Temperature 215 °C
419 °F
Transition Temperature
SK Chemicals SKYTHANE® S375D Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Processing Temperature 215 °C
419 °F
Metering Temperature
SK Chemicals SKYTHANE® S375D Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Processing Temperature 215 - 255 °C
419 - 491 °F
Zhejiang Juner 301-G0 Flammable Resistant
Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, ..
Processing Temperature 215 - 255 °C
419 - 491 °F
Zhejiang Juner 301-G10 10% Glass Fibre Reinforced and Flammable Resistant
Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, ..
Processing Temperature 215 - 260 °C
419 - 500 °F
ExxonMobil PP1222F Mineral-filled Homopolymer
Medium melt flow rate homopolymer, 20% filled. Particularly suitable for consumer products and appliance applications requiring long term heat aging resistance. UL continuous service rating of 95°..
Processing Temperature 215 - 265 °C
419 - 509 °F
E-Polymers Tekaloy® G70NH Non-Halogen Flame Retardant, Un-Reinforced PC/ABS Alloy
Non Halogen Flame Retardant, High FlowInformation provided by E-Polymers Co. Ltd.
Processing Temperature 215 - 225 °C
419 - 437 °F
Injection
Alliance Polymers Zythane™ 3045D Thermoplastic Polyurethane Elastomer
Zythane™ 3045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Processing Temperature 215 - 225 °C
419 - 437 °F
Injection
Alliance Polymers Zythane™ 6055D Thermoplastic Polyurethane Elastomer
Zythane™ 6055D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Processing Temperature 215 °C
419 °F
Gate Temperature; Extrusion
Alliance Polymers Zythane™ 7055D Thermoplastic Polyurethane Elastomer
Zythane™ 7055D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Processing Temperature 215 - 225 °C
419 - 437 °F
Injection
Alliance Polymers Zythane™ 7055D Thermoplastic Polyurethane Elastomer
Zythane™ 7055D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Processing Temperature 215 - 240 °C
419 - 464 °F
Alliance Polymers Viprene™ G50D-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G50D-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Processing Temperature 215 - 232 °C
419 - 450 °F
Preheat
Solvay Specialty Polymers Hylar® MP20 PVDF Polyvinylidene Fluoride  (discontinued **)
Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a..