Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 240 - 245 °C | 464 - 473 °F | Reflow Soldering (Peak) |
Nihon Superior SN100C Lead-Free Solder Alloy Allows high productivity in soldering processes and cost effective, reliable joints. Attributes include high fluidity, low copper erosion, low drossing, superior wetting and freedom from shrinkage d.. |
|||
Processing Temperature | 225 - 245 °C | 437 - 473 °F | |
BASF Elastollan R 1000 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Processing Temperature | 225 - 245 °C | 437 - 473 °F | |
BASF Elastollan R 2001 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Processing Temperature | 225 - 245 °C | 437 - 473 °F | |
BASF Elastollan R 2002 25% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Processing Temperature | 225 - 245 °C | 437 - 473 °F | |
BASF Elastollan R 2005/1 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Processing Temperature | 225 - 245 °C | 437 - 473 °F | |
BASF Elastollan R 2006 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Processing Temperature | 225 - 245 °C | 437 - 473 °F | |
BASF Elastollan R 3000 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Processing Temperature | 225 - 245 °C | 437 - 473 °F | |
BASF Elastollan R 3001 15% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Processing Temperature | 225 - 245 °C | 437 - 473 °F | |
BASF Elastollan R 1001 10% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Processing Temperature | 225 - 245 °C | 437 - 473 °F | |
BASF Elastollan R 2000 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |