Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 232 - 243 °C | 450 - 469 °F | At Nozzle |
Nylene® 401D, Nylon 6 Injection molding grade. Dry as molded. Nylene 401D is a specially formulated nylon 6 molding resin possessing outstanding flow characteristics. Nylene 401D is ideally suited for applications requi.. |
|||
Processing Temperature | 232 - 243 °C | 450 - 469 °F | At Nozzle |
Nylene® 406 Nylon 6, 50% RH Injection molding grade. Nylene 406 is a general purpose, fast cycling molding resin. Crystallization initiators provide fast molding cycles through rapid melt set-up. Parts molded from 406 have bet.. |
|||
Processing Temperature | 232 - 243 °C | 450 - 469 °F | At Nozzle |
Nylene® 406F Nylon 6 Dry as molded. Injection molding grade. Nylene 406F is a resin formulated to comply with FDA regulation 21 CFR 177.1500 for food contact applications. Nylene 406F is a general purpose, fast cycling.. |
|||
Processing Temperature | 232 - 243 °C | 450 - 469 °F | At Nozzle |
Nylene® 406F Nylon 6, 50% RH Injection molding grade. Nylene 406F is a resin formulated to comply with FDA regulation 21 CFR 177.1500 for food contact applications. Nylene 406F is a general purpose, fast cycling molding resin.
.. |
|||
Processing Temperature | 232 - 243 °C | 450 - 469 °F | At Nozzle |
Nylene® 409 Nylon 6, 50% RH Injection molding grade. Nylene 409 is a heat stabilized version of 406 which is a general purpose, fast cycling molding resin. Crystallization initiators provide fast molding cycles through rapid m.. |
|||
Processing Temperature | 232 - 243 °C | 450 - 469 °F | At Nozzle |
Nylene® 452 Nylon 6 Dry as molded. Injection molding grade. Nylene 452 is a plasticized, injection molding nylon for use in applications requiring high flexibility, and excellent toughness and abrasion resistance. Bec.. |
|||
Processing Temperature | 232 °C | 450 °F | |
Chevron Phillips Dynex™ D605A6 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, high antiblock, and processing aid additiveCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, can.. |
|||
Processing Temperature | 232 - 266 °C | 450 - 510 °F | Average value: 249 °C Grade Count:21 |
Overview of materials for Polycarbonate/ABS Alloy, NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, NCG Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Processing Temperature | 232 - 270 °C | 450 - 518 °F | Average value: 251 °C Grade Count:9 |
Overview of materials for Polycarbonate/ABS Alloy, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Carbon Fiber Filled". Each property range of values reported is minimum and max.. |
|||
Processing Temperature | <= 232 °C | <= 450 °F | injection molding |
Chevron Phillips K-Resin® KR03NW Styrene-Butadiene Copolymer, Sheet Grade Styrene-Butadiene Copolymer. No wax (NW) form of K-Resin® KR03 to facilitate printing.Customer Benefits: This SBC is easily processed by injection molding or sheet extrusion and molded parts give .. |
|||
Processing Temperature | 232 - 260 °C | 450 - 500 °F | |
Chevron Phillips Marlex® HHM 5502 BZ High Density Ethylene Hexene Copolymer High Density Ethylene Hexene CopolymerCustomer Benefits: This resin eliminates the need for a mold release agent at machine side. Incorporation of zinc stearate at resin extrusion assures uniform, .. |
|||
Processing Temperature | 232 - 266 °C | 450 - 510 °F | Average value: 249 °C Grade Count:5 |
Overview of materials for PC/ABS + Stainless Steel This property data is a summary of similar materials in the MatWeb database for the category "PC/ABS + Stainless Steel". Each property range of values reported is minimum and maximum values of appro.. |
|||
Processing Temperature | 232 - 257 °C | 450 - 495 °F | Average value: 249 °C Grade Count:9 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is .. |