Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 150 - 210 °C | 302 - 410 °F | |
PolyChem Alloy GMS 2004D Foam Stabilizer PE Foam Stabilizer |
|||
Processing Temperature | 150 °C | 302 °F | Compression or Injection Molding |
Premix Premi-Glas® 1100-15 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100-15 is a fiberglass reinforced thermoset bulk molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent sti.. |
|||
Processing Temperature | 150 °C | 302 °F | Compression Molding |
Premix Premi-Glas® 1200H-10 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200H-10 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.Key features and benefits are:G.. |
|||
Processing Temperature | 150 °C | 302 °F | Compression Molding |
Premix Premi-Glas® 1203-30 Fiberglass Reinforced SMC Description: Premi-Glas® 1203-30 is a fiberglass-reinforced, thermoset sheet molding compound designed for structural and semi-structural components where smooth flat surfaces, high strength and st.. |
|||
Processing Temperature | 150 °C | 302 °F | Compression Molding |
Premix Premi-Glas® 1205 Glass Reinforced SMC Description: Premi-Glas® 1205 is a glass reinforced thermoset Sheet Molding Compound formulated for residential door skins and similar construction applications. Key features and benefits: Excellen.. |
|||
Processing Temperature | 150 °C | 302 °F | Injection or Compression Molding |
Premix Premi-Glas® 2143-24 CR-SX-HT Fiberglass Reinforced Thick Molding Compound Premi-Glas® 2143-24 CR-SX is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves.. |
|||
Processing Temperature | 150 °C | 302 °F | Compression Molding |
Premix Premi-Glas® 2200-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Processing Temperature | 150 °C | 302 °F | Compression Molding |
Premix Premi-Glas® 2203-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2203-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Processing Temperature | 150 °C | 302 °F | Compression Molding |
Premix Premi-Glas® 2203-22 CR-SX-HT Fiberglass Reinforced Thermoset SMC Premi-Glas® 2203-22 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL.. |
|||
Processing Temperature | 150 °C | 302 °F | Compression Molding |
Premix Premi-Glas® 2204-20 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2204-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Good dimensional stability, inclu.. |
|||
Processing Temperature | 150 °C | 302 °F | Compression Molding |
Premix Premi-Glas® 2204-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2204-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Processing Temperature | 150 °C | 302 °F | Injection or Compression Molding |
Premix Premi-Glas® 2243-24 CR-SX Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 2243-24 CR-SX is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves.. |
|||
Processing Temperature | 150 °C | 302 °F | Compression, Transfer or Injection Molding |
Premix Premi-Glas® 3101-10 Fiberglass Reinforced Thermoset BMC Premi-Glas® 3101-10 is a fiberglass reinforced thermoset bulk molding compound for electrical circuit breakers, switchgear and other applications where fire retardance is required.Key features and .. |
|||
Processing Temperature | 150 °C | 302 °F | Compression Molding |
Premix Premi-Glas® 3200-30 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-30 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Processing Temperature | 150 - 170 °C | 302 - 338 °F | Collar Temperature |
Solvay Specialty Polymers Cogegum® GFR/365 Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |
|||
Processing Temperature | 150 - 193 °C | 302 - 379 °F | Average value: 166 °C Grade Count:5 |
Overview of materials for Epoxy, Encapsulating, Glass or Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Glass or Mineral Filled". Each property range of values reported is minimum and ma.. |
|||
Processing Temperature | <= 150 °C | <= 302 °F | Maximum Junction Temperature |
Ferro IP 900 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Si-Pb-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Processing Temperature | 150 - 200 °C | 302 - 392 °F | |
Kraton® D4141 (SBS) Linear Block Copolymer (SBS) styrene-butadiene-styrene block polymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve the impact .. |
|||
Processing Temperature | 150 - 200 °C | 302 - 392 °F | Profiles |
Lucobit Lucobatch® 1850 T10 Polyolefin TPO Granules Lucobatch® 1850 T10 is a highly stabilized polyolefin based TPO granules. Lucobatch® 1850 T10 is employed as a master batch. Blended with suitable polyolefins, tunnel membranes are built of Lu.. |
|||
Processing Temperature | 150 - 180 °C | 302 - 356 °F | Profiles |
Lucobit Lucobit® 1210 Ethylene Copolymer Bitumen Lucobit® combines the positive properties of polyolefins and bitumen. The material is black and consists of mixtures based on high quality polyethylene copolymers with varying additions of speci.. |
|||
Processing Temperature | 150 - 200 °C | 302 - 392 °F | Profiles |
Lucobit Lucofin® 1411-t2 Polyolefin TPO Granules, White Lucofin are colored, highly stabilized polyolefin-based TPO granules. The t2 series is distinguished by good tenacity, high biaxial extensibility and flexibility outstanding breaking strength, and .. |
|||
Processing Temperature | 150 - 200 °C | 302 - 392 °F | Profiles |
Lucobit Lucofin® 1412-t3 Polyolefin TPO Granules, Light Grey Lucofin are colored, highly stabilized polyolefin-based TPO granules. The t3 series is distinguished by good tenacity, high biaxial extensibility and flexibility outstanding breaking strength, and .. |
|||
Processing Temperature | 150 - 180 °C | 302 - 356 °F | Profiles |
Lucobit Lucobit® 1233 Ethylene Copolymer Bitumen Lucobit® combines the positive properties of polyolefins and bitumen. The material is black and consists of mixtures based on high quality polyethylene copolymers with varying additions of speci.. |
|||
Processing Temperature | 150 - 180 °C | 302 - 356 °F | Profiles |
Lucobit Lucofin® 1410-t1 Polyolefin TPO Granules, Grey Lucofin are colored, highly stabilized polyolefin-based TPO granules. The t1 series is distinguished by good tenacity, high biaxial extensibility and flexibility outstanding breaking strength, and .. |
|||
Processing Temperature | 150 - 180 °C | 302 - 356 °F | Profiles |
Lucobit Lucofin® 1413-t1 Polyolefin TPO Granules, Dark Grey Lucofin are colored, highly stabilized polyolefin-based TPO granules. The t1 series is distinguished by good tenacity, high biaxial extensibility and flexibility outstanding breaking strength, and .. |
|||
Processing Temperature | 150 - 180 °C | 302 - 356 °F | Profiles |
Lucobit Lucofin® 1451 Polyolefin TPO Granules, Light Blue Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Processing Temperature | 150 - 180 °C | 302 - 356 °F | |
Total EVA 1005 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1005 VN 4 is made by a high pressure tubular process. Grade for flexible films with high transparency and good mechanical properties. Contains an antioxidant.Application examples: High strengt.. |
|||
Processing Temperature | 150 - 200 °C | 302 - 392 °F | Coating Temperature |
BACT DLC Diamond-Like Coating DLC (a-C:H). This coating provides the highest hardness and abrasion resistance of the BACT products. Typical applications include high wear environments involving seals, molds, metal forming, and.. |
|||
Processing Temperature | 150 - 170 °C | 302 - 338 °F | |
Taiwan Sheen Soon Sheenthane® A9612K Film Grade Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for blown filmInformation provided by Taiwan Sheen Soon Co., LTD. |