Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 180 - 200 °C | 356 - 392 °F | Resin temp |
Asahi Kasei Tenac®-C 8554 Acetal Copolymer, High Flow
(discontinued **) Superhigh-flow grade, with properties necessary for VCR reels.Applications: VCR reels.This product is not a part of the standard product line dated 2003. |
|||
Processing Temperature | 162 - 200 °C | 324 - 392 °F | Forming Temperature |
Kleerdex Vinyloy™ 102 Acrylic/PVC Thermoplastic Sheet
(discontinued **) Recycled capped FR sheetApplications: Vinyloy 102 sheet is capped sheet that can be used to substitute effectively for ABS and other grades of thermoplastic sheet for your thermoforming needs.Featur.. |
|||
Processing Temperature | 160 - 200 °C | 320 - 392 °F | Extrusion cylinder temperature |
LG Chemical KEYFLEX TO-1045D Thermoplastic Olefin for Injection Molding, 45D Hardness KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber .. |
|||
Processing Temperature | 180 - 200 °C | 356 - 392 °F | Tempered and air cooled |
Misumi DC53 JIS Tool Steel General purpose cold work die and mold steel whose strength and toughness approach those of high speed steels. Good machinability and grindability. Tougher than D2 Tool Steel. Machines 30% faster th.. |
|||
Processing Temperature | 150 - 200 °C | 302 - 392 °F | |
Kraton® D4141 (SBS) Linear Block Copolymer (SBS) styrene-butadiene-styrene block polymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve the impact .. |
|||
Processing Temperature | 163 - 200 °C | 325 - 392 °F | Forming Temperature |
KYDEX® 100 Acrylic/PVC Thermoplastic Sheet High impact fire rated sheetApplications: Housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones. Hidden parts for equipment such as vending machines.. |
|||
Processing Temperature | 163 - 200 °C | 325 - 392 °F | Forming |
KYDEX® 6503 Integral Pearlescent Low Heat Release Aviation Thermoforming Sheet Features:Thicknesses from 0.71 mm to 3.18 mmChemical resistant - easy to clean with aggressive cleanersForms deep draws with low forces when heated to the upper end of forming temperature rangeCrisp.. |
|||
Processing Temperature | 163 - 200 °C | 325 - 392 °F | Forming Temperature |
KYDEX® T Acrylic/PVC Thermoplastic Sheet Impact resistant fire rated sheetApplications: External housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones, internal parts for equipment such as v.. |
|||
Processing Temperature | 150 - 200 °C | 302 - 392 °F | Profiles |
Lucobit Lucobatch® 1850 T100 Polyolefin TPO Granules Lucobatch® 1850 T100 is a highly stabilized polyolefin based TPO granules. Lucobatch® 1850 T100 is employed as a master batch. Blended with suitable polyolefins, tunnel membranes are built of .. |
|||
Processing Temperature | 150 - 200 °C | 302 - 392 °F | Profiles |
Lucobit Lucofin® 1412-t3 Polyolefin TPO Granules, Light Grey Lucofin are colored, highly stabilized polyolefin-based TPO granules. The t3 series is distinguished by good tenacity, high biaxial extensibility and flexibility outstanding breaking strength, and .. |
|||
Processing Temperature | 150 - 200 °C | 302 - 392 °F | Profiles |
Lucobit Lucofin® 1413-t3 Polyolefin TPO Granules, Dark Grey Lucofin are colored, highly stabilized polyolefin-based TPO granules. The t3 series is distinguished by good tenacity, high biaxial extensibility and flexibility outstanding breaking strength, and .. |
|||
Processing Temperature | 163 - 200 °C | 325 - 392 °F | Forming Temperature |
KYDEX® 6185 Thermoplastic Sheet High temperature aircraft gradeApplications: Aircraft interior components examples include: air ducts, window reveals, instrument panels, toilet shrouds, armrestsFeatures: Kydex 6185 is a proprietar.. |
|||
Processing Temperature | 180 - 200 °C | 356 - 392 °F | |
Taiwan Sheen Soon Sheenthane® A7630 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Processing Temperature | 180 - 200 °C | 356 - 392 °F | |
Taiwan Sheen Soon Sheenthane® A8630F Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Processing Temperature | 180 - 200 °C | 356 - 392 °F | |
Wanhua Chemical Wanthane® WHT-8170 Polyether-Based TPU Excellent hydrolytic stability, fungus resistance, low temperature flexibility & UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Processing Temperature | 162 - 200 °C | 324 - 392 °F | Forming Temperature |
Kleerdex Kydex® 120 Acrylic/PVC Thermoplastic Sheet
(discontinued **) USDA approved thermoplastic sheetApplications: High impact resistant wallcovering, push plates and kick plates, equipment housings, splash and safety guardsFeatures: Kydex 120 meets class I/A fire c.. |