Polymer Property : Processing Temperature = 370 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 370 °C
698 °F
Average value: 370 °C Grade Count:5
Overview of materials for Polytetrafluoroethylene (PTFE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Molded". Each property range of values reported is minimum and maximum v..
Processing Temperature 370 °C
698 °F
Molding
Azoty Tarnow™ TARFLEN SG-1 PTFE
Free-Flowing suspension powder for automated compression molding of complicated shapes and isostatic pressing.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Processing Temperature 370 °C
698 °F
Molding
Azoty Tarnow™ TARFLEN SG-2 PTFE
Free-Flowing suspension powder for automated compression molding of complicated shapes and isostatic pressing.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Processing Temperature 370 °C
698 °F
Molding
Azoty Tarnow™ TARFLEN SM-1 PTFE
Non Free-Flowing suspension powder for standard compression molding and compounding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Processing Temperature 370 °C
698 °F
Molding
Azoty Tarnow™ TARFLEN SM-2 PTFE
Non Free Flowing suspension powder for standard compression molding and compounding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Processing Temperature 370 °C
698 °F
Molding
Azoty Tarnow™ TARFLEN SM-G15 PTFE
Tarflen SM1 reinforced with 15% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Processing Temperature 370 °C
698 °F
Molding
Azoty Tarnow™ TARFLEN SM-G20 PTFE
Reinforced with 20% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Processing Temperature 370 °C
698 °F
Molding
Azoty Tarnow™ TARFLEN SM-K25 PTFE
Based on Tarflen SM1 reinforced with 25% coke for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Processing Temperature 370 °C
698 °F
Molding
Azoty Tarnow™ TARFLEN SM-S15 PTFE
15% glass fiber reinforced for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Processing Temperature 370 °C
698 °F
Molding
Azoty Tarnow™ TARFLEN SM-S15G2 PTFE
Tarflen SM1 reinforced with 15% glass fibers and 2% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Processing Temperature 370 °C
698 °F
Molding
Azoty Tarnow™ TARFLEN SM-S25 PTFE
Tarflen SM1 reinforced with 25% glass fiber for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Processing Temperature 370 °C
698 °F
Molding
Azoty Tarnow™ TARFLEN ST PTFE
Free-Flowing suspension powder for ram extrusion of rods, pipes and other profiles.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Processing Temperature 370 °C
698 °F
Molding
Azoty Tarnow™ TARFLEN SM-K22G3 PTFE
Tarflen SM1 reinforced with 22% coke and 3% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.