Polymer Property : Processing Temperature = 195 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 195 - 215 °C
383 - 419 °F
Taiwan Sheen Soon Sheenthane® D6050 Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for injection moldingPolyether gradeInformation provided by Taiwan Sheen Soon Co., LTD.
Processing Temperature 195 °C
383 °F
Metering Temperature
SK Chemicals SKYTHANE® CS195A Calendaring Series, Polyether Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Processing Temperature 195 °C
383 °F
Transition Temperature
SK Chemicals SKYTHANE® L185A Polycaprolactone Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Processing Temperature 195 °C
383 °F
Metering Temperature
SK Chemicals SKYTHANE® L185A Polycaprolactone Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Processing Temperature 195 °C
383 °F
Transition Temperature
SK Chemicals SKYTHANE® R190A Polyether Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Processing Temperature 195 °C
383 °F
Metering Temperature
SK Chemicals SKYTHANE® R190A Polyether Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Processing Temperature 195 °C
383 °F
Transition Temperature
SK Chemicals SKYTHANE® S190A Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Processing Temperature 195 °C
383 °F
Transition Temperature
SK Chemicals SKYTHANE® S392A Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Processing Temperature 195 °C
383 °F
Metering Temperature
SK Chemicals SKYTHANE® S392A Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Processing Temperature 195 °C
383 °F
Transition Temperature
SK Chemicals SKYTHANE® X590A Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Processing Temperature 195 °C
383 °F
Metering Temperature
SK Chemicals SKYTHANE® X590A Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Processing Temperature 195 - 215 °C
383 - 419 °F
Wanhua Chemical Wanthane® WHT-1195 Polyester Based TPU
Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd.
Processing Temperature 195 - 215 °C
383 - 419 °F
Wanhua Chemical Wanthane® WHT-1198 Polyester Based TPU
Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd.
Processing Temperature 195 - 210 °C
383 - 410 °F
Wanhua Chemical Wanthane® WHT-1295B Polyester Based TPU
Good mechanical properties, good extrusion stability, low costInformation provided by Wanhua Chemical Group Co., Ltd.
Processing Temperature 195 - 215 °C
383 - 419 °F
Wanhua Chemical Wanthane® WHT-7190 Polycaprolactone Based TPU
Higher mechanical strength, good hydrolytic stability & chemical resistance, weather resistance, heat & fungus resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
Processing Temperature 195 - 215 °C
383 - 419 °F
Wanhua Chemical Wanthane® WHT-8264 Polyether-Based TPU
Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
Processing Temperature 195 - 215 °C
383 - 419 °F
Wanhua Chemical Wanthane® WHT-2198 Polycaprolactone Based TPU
Low compression set, good oil resistance & hydrolytic stability, good abrasion resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd.
Processing Temperature 195 °C
383 °F
Gate Temperature; Extrusion
Alliance Polymers Viprene™ G75A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G75A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Processing Temperature 195 °C
383 °F
Gate Temperature; Extrusion
Alliance Polymers Zythane™ 5070A Thermoplastic Polyurethane Elastomer
Zythane™ 5070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Processing Temperature 195 - 200 °C
383 - 392 °F
Injection
Alliance Polymers Zythane™ 5070A Thermoplastic Polyurethane Elastomer
Zythane™ 5070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Processing Temperature 195 - 200 °C
383 - 392 °F
Injection
Alliance Polymers Zythane™ 6075A Thermoplastic Polyurethane Elastomer
Zythane™ 6075A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Processing Temperature 195 °C
383 °F
Gate Temperature; Extrusion
Alliance Polymers Zythane™ 7070A Thermoplastic Polyurethane Elastomer
Zythane™ 7070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Processing Temperature 195 °C
383 °F
Gate Temperature; Extrusion
Alliance Polymers Viprene™ P70A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P70A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Processing Temperature 195 °C
383 °F
Gate Temperature; Extrusion
Alliance Polymers Viprene™ P70A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P70A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Processing Temperature 195 - 215 °C
383 - 419 °F
Wanhua Chemical Wanthane® WHT-1595 Polyester Based TPU
Low cost, good mechanical properties, good processabilityInformation provided by Wanhua Chemical Group Co., Ltd.
Processing Temperature 195 - 215 °C
383 - 419 °F
Wanhua Chemical Wanthane® WHT-2195 Polycaprolactone Based TPU
Low compression set, good oil resistance & hydrolytic stability, good abrasion resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd.
Processing Temperature 195 - 200 °C
383 - 392 °F
Injection
Alliance Polymers Zythane™ 4070A Thermoplastic Polyurethane Elastomer
Zythane™ 4070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..