Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 154 °C | 309 °F | Optimal Thermoforming temperature for sheet 0.25-1.0 cm (0.10-0.39 in) |
Plaskolite Duraplex® SG-10 Sign Grade Acrylic Sheet, Impact Modified Available in unlimited lengths - no seams in finished products.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Processing Temperature | 154 - 182 °C | 310 - 360 °F | Forming Temp |
Plaskolite Mustang PETG Sheet MUSTANG sheet signage material is continually processed using Eastman Tritan® copolyester, MUSTANG offers superior forming details, improved material distribution and shorter heating and cooling cy.. |
|||
Processing Temperature | 154 - 182 °C | 309 - 360 °F | Thermoforming Surface |
Chevron Phillips Marlex® HXM 50100-02 Extra high molecular weight hexene copolymer
(discontinued **) Benefits: excellent balance of stress cracking resistance, good melt strength, excellent stress cracking resistance, good rigidity, excellent impact strength even at low temperaturesCharacteristics:.. |
|||
Processing Temperature | 154 - 163 °C | 310 - 325 °F | Normal Forming Temperature |
Spartech Polypedic C Polypropylene Copolymer Description: Resilient in cold weather, durable, slightly less rigid than Polypedic OApplications: AFOs; MAFOs; KAFOs; AK and BK sockets; CTLSOs; TLSOs; pelvic bands and joints; pelvic girdles; Info.. |
|||
Processing Temperature | 154 - 163 °C | 310 - 325 °F | Normal Forming Temperature |
Spartech Polypedic O Polypropylene Homopolymer Description: Rigid, strong, fatigue-resistantApplications: AFOs; MAFOs; KAFOs; CTLSOs; TLSOs; pelvic bands and joints; pelvic girdles; AK and BK socketsInformation provided by Spartech. |
|||
Processing Temperature | 154 - 182 °C | 309 - 360 °F | Thermoforming Surface |
Chevron Phillips Marlex® HXM 50100 Extra high molecular weight hexene copolymer Benefits: excellent balance of stress cracking resistance, good melt strength, excellent stress cracking resistance, good rigidity, excellent impact strength even at low temperaturesApplications: 55.. |
|||
Processing Temperature | 154 - 182 °C | 309 - 360 °F | Thermoforming Surface |
Chevron Phillips Marlex® HXM 50100-01 Extra high molecular weight hexene copolymer Benefits: excellent balance of stress cracking resistance, good melt strength, excellent stress cracking resistance, good rigidity, excellent impact strength even at low temperaturesApplications: 55.. |
|||
Processing Temperature | 154 - 315 °C | 309 - 599 °F | Average value: 238 °C Grade Count:4 |
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Coating Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Coating Grade". Each property range of values reported is minimum an.. |
|||
Processing Temperature | 154 °C | 309 °F | Blown Film |
Westlake EMAC® SP 1205 Ethylene-Methyl Acrylate Copolymer
(discontinued **) 20% Methyl Acrylate Content. Characteristics: Processing Temperature Range: 280-600°F, Less Crystalline and Softer than Polyethylene, Excellent Thermal Stability Allows Extrusion Processing up to .. |
|||
Processing Temperature | 154 °C | 309 °F | Blown Film |
Westlake EMAC® SP 1257 Ethylene-Methyl Acrylate Copolymer
(discontinued **) 20% Methyl Acrylate Content. Characteristics: FDA Clearance for Packaging of Most Foods, Including Aseptic Packaging; Less Crystalline and Softer than Polyethylene; Excellent Heat Stability Allows .. |