Spartech Polypedic C Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Spartech
Trade Name Polypedic
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Spartech Polypedic C Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Resilient in cold weather, durable, slightly less rigid than Polypedic OApplications: AFOs; MAFOs; KAFOs; AK and BK sockets; CTLSOs; TLSOs; pelvic bands and joints; pelvic girdles; Information provided by Spartech.
Thermal Properties Metric English Comments
Shrinkage 1.5 - 2.0 %
1.5 - 2.0 %
Processing Properties Metric English Comments
Processing Temperature 87.8 °C
190 °F
Mold and Set Temperature
143 °C
290 °F
Lower Process Limit
154 - 163 °C
310 - 325 °F
Normal Forming Temperature
166 °C
331 °F
Upper Limit Temperature