Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 125 °C | 257 °F | Cure time 45 min at this temperature. |
Momentive Performance Materials RTV6424 White Adhesive Sealant, Non-Corrosive Paste One-part heat cure. Typical uses: Thermal barrier for automotive parts. Fabric seam seal.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of Momentive Performance Materia.. |
|||
Processing Temperature | 125 °C | 257 °F | Cure time 45 min at this temperature. |
Momentive Performance Materials RTV6445 White Adhesive Sealant, Non-Corrosive High Strength Paste One-part heat cure. Typical uses: Thermal barrier for automotive parts. Fabric seam seal.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of Momentive Performance Materia.. |
|||
Processing Temperature | 125 °C | 257 °F | Cure 1.5 hrs |
Aptek 2120 PMF Low modulus urethane staking compound Premixed-frozen, low modulus urethane staking compoundAPTEK 2120-PMF is a one component, premixed-frozen, thixotropic, electrically insulating soft urethane adhesive. It was designed for the stakin.. |
|||
Processing Temperature | 125 °C | 257 °F | Cure 30 min. |
Aptek 2313-PMF Hybrid Epoxy Adhesive Snap-cure, silver-filled; long pot-life/stable viscosity-excellent for robotics. Thermal shock resistant.Production-oriented, snap-cure technology for surface mount applications-allows cure during s.. |
|||
Processing Temperature | 125 °C | 257 °F | Cure 2 hrs |
Aptek 2503R-A/B Premeasured conformal urethane coating repair kit APTEK 2503-A/B is an unfilled, two component, electrically insulating, transparent, flexible urethane coating system designed for the encapsulation and protection of electrical/electronic components.. |
|||
Processing Temperature | 125 °C | 257 °F | Cure 0.5 hrs |
Aptek 6512-PMF Electronic grade, conductive epoxy adhesive APTEK 6512-PMF is a one component, 100% solid, silver-filled, electrically conductive epoxy adhesive specifically designed for the attachment of electronic components to printed circuit boards. APT.. |
|||
Processing Temperature | 125 °C | 257 °F | Suggested baking time at this temperature is 1-5 hr. |
Von Roll Isola IMI Varnish 3405 Polyester Varnish for Electrical Insulation Data provided by Von Roll Isola USA.Flash Point: |