Momentive Performance Materials RTV6424 White Adhesive Sealant, Non-Corrosive Paste

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Momentive Performance Materials (Former GE Silicones)
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Momentive Performance Materials RTV6424 White Adhesive Sealant, Non-Corrosive Paste.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
One-part heat cure. Typical uses: Thermal barrier for automotive parts. Fabric seam seal.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of Momentive Performance Materials in 2006.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore A 30
30
Tensile Strength, Ultimate 4.65 MPa
674 psi
Elongation at Break 550 %
550 %
Electrical Properties Metric English Comments
Dielectric Constant 2.9
2.9
Dielectric Strength 19.5 kV/mm
495 kV/in
Processing Properties Metric English Comments
Processing Temperature 125 °C
257 °F
Cure time 45 min at this temperature.