Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 120 - 160 °C | 248 - 320 °F | Sheet Forming |
Polycasa COPOL PETG QUINN COPOL has good optical properties, brilliant surface, easy to vacuum form without pre-drying, low water absorption, very good chemical resistance, and high impact properties.Bus shelters (UV-v.. |
|||
Processing Temperature | 120 - 160 °C | 248 - 320 °F | Sheet Forming |
Polycasa LENTICULAR PETG Good ink adhesionGood receptabilityStable sheet dimensionsHigh impact strengthGood chemical resistanceEnvironmentally safeRecyclableMeets current food contact legislationDisplays Graphic Arts Advert.. |
|||
Processing Temperature | 120 - 160 °C | 248 - 320 °F | Sheet Forming |
Polycasa PETG QUINN PETG has good optical properties and a brilliant surface. The PETG range of sheets are easy to fabricate, to vacuum form, and show exceptional low temperature performance. Important benefits o.. |
|||
Processing Temperature | 120 °C | 248 °F | Cure Schedule: 2 hrs @ 120ºC, 6 hrs @ 150°C, or 2 hrs @ 190°C |
Huntsman DY 9577 Epoxy Accelerator Mix Ratio with GY 6010 is 1.Comments/Applications: Casting, encapsulation, powder coatings, filament windings, pultrusion, molding, electrical tapes. Can be used as a catalyst. Latent at RT in GY.. |
|||
Processing Temperature | 120 °C | 248 °F | Cure Schedule: 2 hrs @ 120ºC, 6 hrs @ 150°C, or 2 hrs @ 190°C |
Huntsman DY 9577 Special Hardener Mix Ratio with 100 phr GY 6010 is 1.Comments/Applications: Latent catalytic curing agent for liquid epoxy resins or as a latent accelerator for anhydride cured epoxy resins. Latent at RT in GY 601.. |
|||
Processing Temperature | 120 °C | 248 °F | Cure Schedule: 15 min @ 120°C |
Huntsman HT 3261 Special Hardener Mix Ratio with 100 phr GT 70130 is 6.Comments/Applications: Solid resinous amino-containing hardener. *Mix ratio with Araldite GT 7013. For low temperature cure, high gloss. Decorative and prote.. |
|||
Processing Temperature | 120 - 150 °C | 248 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 0600 Unsaturated Polyester UP SMC 0600 is a specially formulated SMC for reduced moulding pressure (< 30 bar). The glass level has been selected to combine good mouldability with strength and stiffness. Even without a specific f.. |
|||
Processing Temperature | 120 - 150 °C | 248 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 0650 Unsaturated Polyester UP SMC 0650 Low pressure SMC for large panels when moulding force becomes critical. Specific moulding pressure < 20 bar. A Special molding procedure is necessary.Information Provided by Menzolit |
|||
Processing Temperature | 120 - 150 °C | 248 - 302 °F | |
Gwent Electronic Materials C2010515D4 Silver Ink Silver Ink C2010515D4 is designed as an internal electrode ink for LTCC applications. It is compatible with other members of the GEM range of Silver LTCC Inks and most LTCC tape systems on the mark.. |
|||
Processing Temperature | 120 - 150 °C | 248 - 302 °F | |
Gwent Electronic Materials C2031105D2 Palladium Ink Palladium Ink C2031105D2 is an ink formulated for screen printing for use on Fuel Cells. It is suitable for application onto Solid Oxide Fuel Cells.The ink has been made at a ready to use viscosity.. |
|||
Processing Temperature | 120 °C | 248 °F | Suggested baking time at this temperature is 0.75 hr. May also be cured for shorter time at higher temperatures. |
Von Roll Isola IMI E-Solder® 3017 Electrically Conductive Adhesive Data provided by Von Roll Isola USA.E-SOLDER® epoxy based resin systems can be used at room temperature on heat sensitive materials, can bond dissimilar materials, and do not have flux or residue t.. |
|||
Processing Temperature | 120 - 150 °C | 248 - 302 °F | Glue Line Temperature |
EMS-Griltech Griltex® 11A Copolyamide Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Processing Temperature | 120 - 150 °C | 248 - 302 °F | Lamination Adhesive |
EMS-Griltech Griltex® 11A Copolyamide Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Processing Temperature | 120 - 150 °C | 248 - 302 °F | Glue Line Temperature |
EMS-Griltech Griltex® D 1260 A Copolyamide Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Processing Temperature | 120 - 140 °C | 248 - 284 °F | Glue Line Temperature |
EMS-Griltech Griltex® D 1365E Copolyester Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Processing Temperature | 120 - 160 °C | 248 - 320 °F | Films Die Head |
EMS-Griltech Griltex® D 1442E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Processing Temperature | 120 - 140 °C | 248 - 284 °F | Lamination Adhesive |
EMS-Griltech Griltex® D 1539E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Processing Temperature | 120 - 200 °C | 248 - 392 °F | |
Fainplast Compounds Hax™ HFX 500 Crosslinkable HFFR Cable Compound Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Standard sheathingInformation provided by Fainplast Compou.. |
|||
Processing Temperature | 120 - 200 °C | 248 - 392 °F | |
Fainplast Compounds Hax™ HFX 500S Crosslinkable HFFR Cable Compound Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Sheathing for solar cablesInformation provided by Fainplas.. |
|||
Processing Temperature | 120 - 200 °C | 248 - 392 °F | |
Fainplast Compounds Hax™ HFX 505 Crosslinkable HFFR Cable Compound Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Sheathing; InsulationInformation provided by Fainplast Com.. |
|||
Processing Temperature | 120 - 200 °C | 248 - 392 °F | |
Fainplast Compounds Hax™ HFX 509 Crosslinkable HFFR Cable Compound Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Insulation for solar cablesInformation provided by Fainpla.. |
|||
Processing Temperature | 120 - 200 °C | 248 - 392 °F | |
Fainplast Compounds Hax™ HFX 515 Crosslinkable HFFR Cable Compound Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Sheathing, InsulationInformation provided by Fainplast Com.. |
|||
Processing Temperature | 120 - 200 °C | 248 - 392 °F | |
Fainplast Compounds Hax™ HFX 519 Crosslinkable HFFR Cable Compound Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Sheathing, InsulationInformation provided by Fainplast Com.. |
|||
Processing Temperature | 120 - 200 °C | 248 - 392 °F | |
Fainplast Compounds Hax™ HFX 521 Crosslinkable HFFR Cable Compound Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Oil resistant sheathingInformation provided by Fainplast C.. |
|||
Processing Temperature | 120 °C | 248 °F | Cure 1.5 hrs |
Aptek 2503-A/B Low modulus urethane conformal coating APTEK 2503-A/B is an unfilled, two component, electrically insulating, transparent, flexible urethane coating system designed for the encapsulation and protection of electronic services mounted on p.. |
|||
Processing Temperature | 120 - 150 °C | 248 - 302 °F | |
Gwent Electronic Materials C2010809D3 Silver Ink Silver Ink C2010809D3 is designed for printing via, when screen printed onto LTCC tape. It is compatible with other members of the GEM range of Silver LTCC Inks and most LTCC tape systems on the ma.. |
|||
Processing Temperature | 120 - 268 °C | 248 - 514 °F | Average value: 217 °C Grade Count:15 |
Overview of materials for Polypropylene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of.. |