Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 2.25 J/g-°C @Temperature 20.0 - 150 °C |
0.538 BTU/lb-°F @Temperature 68.0 - 302 °F |
|
DSM Akulon® F127 PA6 Low/Medium Viscosity, Film Extrusion |
|||
Specific Heat Capacity | 2.25 J/g-°C @Temperature 20.0 - 150 °C |
0.538 BTU/lb-°F @Temperature 68.0 - 302 °F |
|
DSM Akulon® F130 PA6 Film Extrusion, Medium Viscosity |
|||
Specific Heat Capacity | 2.25 J/g-°C @Temperature 20.0 - 150 °C |
0.538 BTU/lb-°F @Temperature 68.0 - 302 °F |
|
DSM Akulon® F130-C2 PA6 Medium Viscosity, Film Extrusion, Lubricated |
|||
Specific Heat Capacity | 2.25 J/g-°C @Temperature 20.0 - 150 °C |
0.538 BTU/lb-°F @Temperature 68.0 - 302 °F |
|
DSM Akulon® F130-C3 PA6 Monofilament Grade, Extrusion Grade, Medium Viscosity, Lubricated |
|||
Specific Heat Capacity | 2.25 J/g-°C @Temperature 20.0 - 150 °C |
0.538 BTU/lb-°F @Temperature 68.0 - 302 °F |
|
DSM Akulon® F130-E1 PA6 Medium Viscosity, Nucleated, Lubricated, Film Extrusion |
|||
Specific Heat Capacity | 2.25 J/g-°C @Temperature 20.0 - 150 °C |
0.538 BTU/lb-°F @Temperature 68.0 - 302 °F |
|
DSM Akulon® F130-E5 PA6 Medium Viscosity, Nucleated, Lubricated, Film Extrusion, Antiblock |
|||
Specific Heat Capacity | 2.25 J/g-°C @Temperature 20.0 - 150 °C |
0.538 BTU/lb-°F @Temperature 68.0 - 302 °F |
|
DSM Akulon® F132-C1 PA6 Film Extrusion, High Viscosity, Lubricated |
|||
Specific Heat Capacity | 2.25 J/g-°C @Temperature 20.0 - 150 °C |
0.538 BTU/lb-°F @Temperature 68.0 - 302 °F |
|
DSM Akulon® F132-E1 PA6 Medium/High Viscosity, Nucleated, Lubricated, Film Extrusion |
|||
Specific Heat Capacity | 2.25 J/g-°C @Temperature 20.0 - 150 °C |
0.538 BTU/lb-°F @Temperature 68.0 - 302 °F |
|
DSM Akulon® F132-E2 PA6 High Viscosity, Nucleated, Lubricated, Film Extrusion |
|||
Specific Heat Capacity | 2.25 J/g-°C @Temperature 20.0 - 150 °C |
0.538 BTU/lb-°F @Temperature 68.0 - 302 °F |
|
DSM Akulon® F136 PA6 Very High Viscosity, Film Extrusion |
|||
Specific Heat Capacity | 2.25 J/g-°C @Temperature 20.0 - 150 °C |
0.538 BTU/lb-°F @Temperature 68.0 - 302 °F |
|
DSM Akulon® F136-C PA6 Film Extrusion, Very High Viscosity, Lubricated |
|||
Specific Heat Capacity | 2.25 J/g-°C @Temperature 20.0 - 150 °C |
0.538 BTU/lb-°F @Temperature 68.0 - 302 °F |
|
DSM Akulon® F136-C1 PA6 Very High Viscosity, Film Extrusion, Lubricated |
|||
Specific Heat Capacity | 2.25 J/g-°C @Temperature 20.0 - 150 °C |
0.538 BTU/lb-°F @Temperature 68.0 - 302 °F |
|
DSM Akulon® F136-E1 PA6 Very High Viscosity, Lubricated, Nucleated, Film Extrusion |
|||
Specific Heat Capacity | 2.25 J/g-°C @Temperature 20.0 - 150 °C |
0.538 BTU/lb-°F @Temperature 68.0 - 302 °F |
|
DSM Akulon® F136-E2 PA6 Very High Viscosity, Lubricated, Nucleated, Film Extrusion |
|||
Specific Heat Capacity | 2.25 J/g-°C @Temperature 20.0 - 150 °C |
0.538 BTU/lb-°F @Temperature 68.0 - 302 °F |
|
DSM Akulon® F234-C PA6 Film Extrusion, High Viscosity, Lubricated |
|||
Specific Heat Capacity | 2.25 J/g-°C @Temperature 20.0 - 150 °C |
0.538 BTU/lb-°F @Temperature 68.0 - 302 °F |
|
DSM Akulon® XP36-C1 PA6 Film Extrusion, Medium Viscosity, Lubricated |
|||
Specific Heat Capacity | 2.25 J/g-°C @Temperature 20.0 - 150 °C |
0.538 BTU/lb-°F @Temperature 68.0 - 302 °F |
|
DSM Akulon® F128 PA6 Film Extrusion, Medium Viscosity |
|||
Specific Heat Capacity | 2.25 J/g-°C @Temperature 20.0 - 150 °C |
0.538 BTU/lb-°F @Temperature 68.0 - 302 °F |
|
DSM Akulon® XP32-C1 PA6 Film Extrusion, Medium Viscosity, Lubricated |
|||
Specific Heat Capacity | 2.25 J/g-°C @Temperature 20.0 - 150 °C |
0.538 BTU/lb-°F @Temperature 68.0 - 302 °F |
|
DSM Akulon® XP36-E1 PA6 Film Extrusion, Medium Viscosity, Nucleated, Lubricated |