Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.27 J/g-°C @Temperature 50.0 °C |
0.304 BTU/lb-°F @Temperature 122 °F |
DSC |
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 resin. .. |
|||
Specific Heat Capacity | 1.27 J/g-°C @Temperature 50.0 °C |
0.304 BTU/lb-°F @Temperature 122 °F |
ASTM C351 |
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 res.. |