Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 2.05 J/g-°C @Temperature 280 °C |
0.490 BTU/lb-°F @Temperature 536 °F |
|
Pearl Engineering PEPLPET B-105C PET Bottle Grade A co-polymer used for soft drinks and other applications. |
|||
Specific Heat Capacity | 2.05 J/g-°C @Temperature 280 °C |
0.490 BTU/lb-°F @Temperature 536 °F |
|
Pearl Engineering PEPLPET B-109JS PET Sheet Grade Used mainly for 5 to 20 liter mineral water containers |
|||
Specific Heat Capacity | 2.05 J/g-°C @Temperature 280 °C |
0.490 BTU/lb-°F @Temperature 536 °F |
|
Pearl Engineering PEPLPET B-113C PET Sheet Grade Used mainly for box strapping. |
|||
Specific Heat Capacity | 2.05 J/g-°C @Temperature 280 °C |
0.490 BTU/lb-°F @Temperature 536 °F |
|
Pearl Engineering PEPLPET D-101-SH Monofilament Resin Used in the paper industry as paper pulp nets. |
|||
Specific Heat Capacity | 2.05 J/g-°C @Temperature 280 °C |
0.490 BTU/lb-°F @Temperature 536 °F |
|
Pearl Engineering PEPLPET F096H Film Grade Resin Used mainly as PET films/ sheets, known as Superbright |
|||
Specific Heat Capacity | 2.05 J/g-°C @Temperature 280 °C |
0.490 BTU/lb-°F @Temperature 536 °F |
|
Pearl Engineering PEPLPET F096HA Film Grade Resin Used mainly as PET films/ sheets, known as bright with anti-blocking agent. |
|||
Specific Heat Capacity | 2.05 J/g-°C @Temperature 280 °C |
0.490 BTU/lb-°F @Temperature 536 °F |
|
Pearl Engineering PEPLPET F097H Film Grade Resin Used mainly as PET films/ sheets, known as Superbright |
|||
Specific Heat Capacity | 2.05 J/g-°C @Temperature 280 °C |
0.490 BTU/lb-°F @Temperature 536 °F |
|
Pearl Engineering PEPLPET F097HA Film Grade Resin Used mainly as PET films/ sheets, known as bright with anti-blocking agent. |
|||
Specific Heat Capacity | 2.05 J/g-°C @Temperature 280 °C |
0.490 BTU/lb-°F @Temperature 536 °F |
|
Pearl Engineering PEPLPET FR-101-H Monofilament Resin Used as textile grade flame retardant for furniture, car and plane upholstery. |
|||
Specific Heat Capacity | 2.05 J/g-°C @Temperature 250 °C |
0.490 BTU/lb-°F @Temperature 482 °F |
|
Eastman EASTALLOY Polymer DA003-8999K, Clear Alloy
(discontinued **) Properties below based on a film thickness of 250 microns. CO2 Permeability is 49 cm3·mm/m2·24h·atm per ASTM D 1434.Product Description: EASTALLOY DA003-8999K Polymer is a clear copolyester/pol.. |
|||
Specific Heat Capacity | 2.05 J/g-°C @Temperature 280 °C |
0.490 BTU/lb-°F @Temperature 536 °F |
|
Pearl Engineering PEPLPET B-07C PET Bottle Grade A co-polymer used mostly for containers. |
|||
Specific Heat Capacity | 2.05 J/g-°C @Temperature 280 °C |
0.490 BTU/lb-°F @Temperature 536 °F |
|
Pearl Engineering PEPLPET B-101C PET Sheet Grade A sheet grade polymer used in thick films. |
|||
Specific Heat Capacity | 2.05 J/g-°C @Temperature 280 °C |
0.490 BTU/lb-°F @Temperature 536 °F |
|
Pearl Engineering PEPLPET B101H Monofilament Resin Generally used in monofilament v-belts, zips and other technical applications. |
|||
Specific Heat Capacity | 2.05 J/g-°C @Temperature 280 °C |
0.490 BTU/lb-°F @Temperature 536 °F |
|
Pearl Engineering PEPLPET B-103C PET Bottle Grade A co-polymer used for mineral water bottles |
|||
Specific Heat Capacity | 2.05 J/g-°C @Temperature 250 °C |
0.490 BTU/lb-°F @Temperature 482 °F |
DSC |
Eastman Cadence™ GS1 Copolyester for film calendering Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe.. |
|||
Specific Heat Capacity | 2.05 J/g-°C @Temperature 250 °C |
0.490 BTU/lb-°F @Temperature 482 °F |
DSC |
Eastman Cadence™ GS2 Copolyester for film calendering Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe.. |
|||
Specific Heat Capacity | 2.05 J/g-°C @Temperature 250 °C |
0.490 BTU/lb-°F @Temperature 482 °F |
DSC |
Eastman Cadence™ GS3 Copolyester for film calendering Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe.. |
|||
Specific Heat Capacity | 2.05 J/g-°C @Temperature 250 °C |
0.490 BTU/lb-°F @Temperature 482 °F |
DSC |
Eastman Cadence™ GS4 Copolyester for film calendering Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe.. |
|||
Specific Heat Capacity | 2.05 J/g-°C @Temperature 250 °C |
0.490 BTU/lb-°F @Temperature 482 °F |
DSC |
Eastman Drystar 0601 Copolyester, Injection Molded This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen.. |
|||
Specific Heat Capacity | 2.05 J/g-°C @Temperature 240 °C |
0.490 BTU/lb-°F @Temperature 464 °F |
DSC |
Eastman Eastar MN004 Copolyester Eastar Copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar MN004 contains a mold release.Appl.. |
|||
Specific Heat Capacity | 2.05 J/g-°C @Temperature 250 °C |
0.490 BTU/lb-°F @Temperature 482 °F |
DSC |
Eastman Eastman 1223 Copolyester Applications:Blown filmCredit cardsDebit cardsDeodorant packagingElectronic packagingFabricated boxesFlexible packagingFood packagingFurniture/Furniture trimGaming cardsGift cardsIdentification card.. |