Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.673 J/g-°C @Temperature 1100 °C |
0.161 BTU/lb-°F @Temperature 2010 °F |
|
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1093°C 1 hr Data provided by Carpenter Technology Corporation.Annealing followed by water quench and low stress grinding prior to tensile testing.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting h.. |
|||
Specific Heat Capacity | 0.673 J/g-°C @Temperature 1100 °C |
0.161 BTU/lb-°F @Temperature 2010 °F |
|
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1093°C 2 hr Data provided by Carpenter Technology Corporation.Annealing followed by water quench and low stress grinding prior to tensile testing.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting h.. |
|||
Specific Heat Capacity | 0.673 J/g-°C @Temperature 1100 °C |
0.161 BTU/lb-°F @Temperature 2010 °F |
|
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1121°C 1 hr Data provided by Carpenter Technology Corporation.Annealing followed by water quench and low stress grinding prior to tensile testing.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting h.. |
|||
Specific Heat Capacity | 0.673 J/g-°C @Temperature 1100 °C |
0.161 BTU/lb-°F @Temperature 2010 °F |
|
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1149°C (2100°F) 1 hr Data provided by Carpenter Technology Corporation.Annealing followed by water quench and low stress grinding prior to tensile testing.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting h.. |
|||
Specific Heat Capacity | 0.673 J/g-°C @Temperature 1100 °C |
0.161 BTU/lb-°F @Temperature 2010 °F |
|
Carpenter BioDur™ CCM® Medical Implant Alloy, Annealed Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting high strength, corrosion resistance, and wear resistance. BioDur Carpenter CCM alloy.. |
|||
Specific Heat Capacity | 0.673 J/g-°C @Temperature 1100 °C |
0.161 BTU/lb-°F @Temperature 2010 °F |
|
Carpenter BioDur™ CCM® Medical Implant Alloy, Warm Worked Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting high strength, corrosion resistance, and wear resistance. BioDur Carpenter CCM alloy.. |
|||
Specific Heat Capacity | 0.673 J/g-°C @Temperature 1100 °C |
0.161 BTU/lb-°F @Temperature 2010 °F |
|
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Hot Worked Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting high strength, corrosion resistance, and wear resistance. BioDur CCM Plus alloy is a.. |
|||
Specific Heat Capacity | 0.673 J/g-°C @Temperature 1100 °C |
0.161 BTU/lb-°F @Temperature 2010 °F |
|
Carpenter BioDur™ CCM® Medical Implant Alloy, Hot Worked Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting high strength, corrosion resistance, and wear resistance. BioDur Carpenter CCM alloy.. |