Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 160 µm/m-°C @Temperature 150 - 250 °C |
88.9 µin/in-°F @Temperature 302 - 482 °F |
ASTM E831 |
Solvay Specialty Polymers Amodel® A-4122 HR WH 117 Polyphthalamide (PPA)
(Unverified Data**) Amodel A-4122 HR resin is a 22% glass reinforced polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material exhibits high heat resistance, high st.. |
|||
CTE, linear, Transverse to Flow | 160 µm/m-°C @Temperature 55.0 - 100 °C |
88.9 µin/in-°F @Temperature 131 - 212 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 100TL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100TL NC010 is a high viscosity acetal homopolymer with 1.5% Teflon® PTFE Micropowder.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 160 µm/m-°C @Temperature 55.0 - 100 °C |
88.9 µin/in-°F @Temperature 131 - 212 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 127UV BK701 Acetal Homopolymer
(Unverified Data**) Delrin® 127UV BK701 is a high viscosity, UV stabilized acetal homopolymer. It has excellent impact strength, UV resistance and thermal stability. It is well suited for automotive interior applicati.. |
|||
CTE, linear, Transverse to Flow | 160 µm/m-°C @Temperature 55.0 - 100 °C |
88.9 µin/in-°F @Temperature 131 - 212 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 300CP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of processing and part performance.Information provided by DuPont Perf.. |
|||
CTE, linear, Transverse to Flow | 160 µm/m-°C @Temperature 55.0 - 100 °C |
88.9 µin/in-°F @Temperature 131 - 212 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 527UV BK701 Acetal Homopolymer
(Unverified Data**) Delrin® 527UV BK701 is a medium viscosity black acetal homopolymer resin with UV stabilizers developed for automotive interior applications. It has improvements in UV aging characteristics and ther.. |
|||
CTE, linear, Transverse to Flow | 160 µm/m-°C @Temperature 55.0 - 100 °C |
88.9 µin/in-°F @Temperature 131 - 212 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® FG500P NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG500P is a medium viscosity acetal homopolymer, with improved thermal stability. It has been developed for consideration into applications such as parts for the food industry.Information p.. |
|||
CTE, linear, Transverse to Flow | 160 µm/m-°C @Temperature 100 - 250 °C |
88.9 µin/in-°F @Temperature 212 - 482 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® A-4122 HR WH 117 Polyphthalamide (PPA), 22% Glass Fiber Amodel® A-4122 HR resin is a 22% glass reinforced polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material exhibits high heat resistance, hig.. |
|||
CTE, linear, Transverse to Flow | 160 µm/m-°C @Temperature 55.0 - 100 °C |
88.9 µin/in-°F @Temperature 131 - 212 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 300PE NC010A Acetal Homopolymer Delrin® 300PE NC010A is a medium-high viscosity acetal homopolymer, an enhanced version with extremely low VOC emissions. It has improved processing thermal stability, good mechanical properties, a.. |
|||
CTE, linear, Transverse to Flow | 160 µm/m-°C @Temperature 55.0 - 100 °C |
88.9 µin/in-°F @Temperature 131 - 212 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 500PE NC010A Acetal Homopolymer Delrin® 500PE NC010A is a medium viscosity acetal homopolymer, an enhanced version of Delrin® 500P with extremely low VOC emissions. It has improved processing thermal stability, and good mechanic.. |
|||
CTE, linear, Transverse to Flow | 160 µm/m-°C @Temperature 55.0 - 100 °C |
88.9 µin/in-°F @Temperature 131 - 212 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 100PE NC010A Acetal Homopolymer Delrin® 100PE NC010A is a high viscosity acetal homopolymer, an enhanced version of Delrin® 100P with extremely low VOC emissions. It has improved processing thermal stability, good mechanical pro.. |
|||
CTE, linear, Transverse to Flow | 160 µm/m-°C @Temperature 55.0 - 100 °C |
88.9 µin/in-°F @Temperature 131 - 212 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® FG100TL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100TL is a high viscosity acetal homopolymer, containing 1.5% Teflon® PTFE Micropowder. It has been developed for consideration into applications such as parts for the food industry.Inform.. |
|||
CTE, linear, Transverse to Flow | 160 µm/m-°C @Temperature 23.0 - 80.0 °C |
88.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® VX4510 PBT (Europe-Africa-Middle East) VALOX VX4510 is a flame retarded, 10% glassfiber reinforced injection moulding PBT resin. |