Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 945ASR PC Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t.. |
|||
CTE, linear, Transverse to Flow | 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 945ASR PC (Asia Pacific) Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t.. |
|||
CTE, linear, Transverse to Flow | 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 945ASR PC (Europe-Africa-Middle East) Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t.. |
|||
CTE, linear, Transverse to Flow | 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Lubricomp CI001 PS LNP* Lubricomp* CI001 is a compound based on Polystyrene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the America.. |
|||
CTE, linear, Transverse to Flow | 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP DX98306H PC LNP* LUBRICOMP* DX98306H is a compound based on Polycarbonate resin containing Proprietary Fillers. Added features of this material include: Wear Resistant, Low Extractible. |
|||
CTE, linear, Transverse to Flow | 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP DX98306H PC (Asia Pacific) LNP* Lubricomp* DX98306H is a compound based on Polycarbonate resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
CTE, linear, Transverse to Flow | 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP RX03643H PA 66 LNP* LUBRICOMP* RX03643H is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP RX03643H PA 66 (Asia Pacific) LNP* Lubricomp* RX03643H is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRILOY D2000 PC (Asia Pacific) LNP LUBRILOY* D2000 is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRILOY D2000 PC (Asia Pacific) LNP LUBRILOY* D2000 is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRILOY D2000AXH PC LNP LUBRILOY* D2000AXH is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare. |
|||
CTE, linear, Transverse to Flow | 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRILOY D2000AXH PC LNP LUBRILOY* D2000AXH is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare. |
|||
CTE, linear, Transverse to Flow | 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Lubriloy D2000XXH PC LNP LUBRILOY* D2000XXH is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated, Healthcare.This data was supplied.. |
|||
CTE, linear, Transverse to Flow | 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubriloy D2000XXH PC LNP LUBRILOY* D2000XXH is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated, Healthcare.This data was supplied.. |
|||
CTE, linear, Transverse to Flow | 73.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® 1760 PBT+PC 11% Glass Reinforced PBT+PC alloy. Impact/chemical resistant. Excellent physical property retention in automotive exteriors. |
|||
CTE, linear, Transverse to Flow | 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Thermocomp IF006S PA 6/12 (Asia Pacific) LNP* Thermocomp* IF006S is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia Paci.. |
|||
CTE, linear, Transverse to Flow | 73.8 µm/m-°C @Temperature 25.6 - 93.3 °C |
41.0 µin/in-°F @Temperature 78.0 - 200 °F |
Diameter |
Saint-Gobain Rulon® 641 Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
CTE, linear, Transverse to Flow | 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP QFL36 PA 6/10 LNP LUBRICOMP* QFL36 is a compound based on Nylon 6/10 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Lubricomp CI001 PS (Asia Pacific) LNP* Lubricomp* CI001 is a compound based on Polystyrene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pa.. |
|||
CTE, linear, Transverse to Flow | 73.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Thermocomp IF006S PA6.12 LNP* Thermocomp* IF006S is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas .. |