Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 66.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL1036 PC Copolymer Lexan* EXL1036 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high viscosity grade designed for (co-)extrusion. This resin offers extreme low temperature (-60 C) ductility and good h.. |
|||
CTE, linear, Transverse to Flow | 66.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL1036 PC Copolymer (Asia Pacific) Lexan* EXL1036 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high viscosity grade designed for (co-)extrusion. This resin offers extreme low temperature (-60 C) ductility and good h.. |
|||
CTE, linear, Transverse to Flow | 66.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL1036 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1036 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high viscosity grade designed for (co-)extrusion. This resin offers extreme low temperature (-60 C) ductility and good h.. |
|||
CTE, linear, Transverse to Flow | 66.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer Lexan* EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in .. |
|||
CTE, linear, Transverse to Flow | 66.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer (Asia Pacific) Lexan* EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in .. |
|||
CTE, linear, Transverse to Flow | 66.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in .. |
|||
CTE, linear, Transverse to Flow | 66.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL9330P PC COPOLYMER (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA. |
|||
CTE, linear, Transverse to Flow | 66.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA. |
|||
CTE, linear, Transverse to Flow | 66.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA. |
|||
CTE, linear, Transverse to Flow | 66.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA. |
|||
CTE, linear, Transverse to Flow | 66.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Lubricomp KCL22 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KCL22 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data .. |
|||
CTE, linear, Transverse to Flow | 66.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Lubriloy D20001 PC LNP LUBRILOY* D20001 is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Flame Retardant.This data was supplied by.. |
|||
CTE, linear, Transverse to Flow | 66.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRILOY D20001 PC (Asia Pacific) LNP LUBRILOY* D20001 is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Flame Retardant. |
|||
CTE, linear, Transverse to Flow | 66.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Lubricomp KCL22 Acetal Copoly LNP* Lubricomp* KCL22 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data .. |