Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 52.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON DD0001 PC LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
CTE, linear, Transverse to Flow | 52.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON DD0001 PC (Asia Pacific) LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 52.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON DD0001 PC (Europe-Africa-Middle East) LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 52.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP 9X04488 POLYPHENYLENESULFONE (Asia Pacific) LNP* Thermocomp* 9X04488 is a compound based on POLYPHENYLENESULFONE resin containing Mineral. |
|||
CTE, linear, Transverse to Flow | 52.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP 9X04488 PPS LNP* THERMOCOMP* 9X04488 is a compound based on PPS resin containing Mineral. |
|||
CTE, linear, Transverse to Flow | 52.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp 9X04488 POLYPHENYLENESULFONE LNP* Thermocomp* 9X04488 is a compound based on POLYPHENYLENESULFONE resin containing Mineral.This data was supplied by SABIC-IP for the Americas region. |