Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Parallel to Flow = 10.6 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature 160 - 250 °C
10.6 µin/in-°F

@Temperature 320 - 482 °F
Solvay Specialty Polymers Amodel® A-1340 HS Polyphthalamide (PPA) Resin, 40% Mineral/Glass Reinforced, Dry as Molded &a
AMODEL® A-1340 HS is a 40% mineral/glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, high tensile strength and low warpage..
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature 0.000 - 100 °C
10.6 µin/in-°F

@Temperature 32.0 - 212 °F
2
Solvay Specialty Polymers Amodel® A-1133 L WH 015 Polyphthalamide (PPA), 33% Glass Fiber
Formerly referred to as Amodel® PXM-13015. Amodel® A-1133 L resin is a 33% glass reinforced polyphthalamide (PPA) which is distinguished by its high-reflectivity white color. This grade featu..
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature 150 - 250 °C
10.6 µin/in-°F

@Temperature 302 - 482 °F
2
Solvay Specialty Polymers Amodel® A-4122 LS WH678 Polyphthalamide (PPA), 22% Glass Fiber
Amodel® A-4122 LS is a 22% glass fiber reinforced, light-stabilized, high-reflectivity white grade of Amodel polyphthalamide (PPA). It is designed to provide high crystallinity when molded in wat..
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature 200 - 250 °C
10.6 µin/in-°F

@Temperature 392 - 482 °F
4
Solvay Specialty Polymers Lavanta® 5115 WH 011 Polyester, High Performance (HPP), 15% Glass Fiber
Lavanta® 5115 WH011 is a 15% glass fiber reinforced, high-performance polyester (HPP) injection molding grade developed specifically for HB LED packaging applications that utilize surface mount ..
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
10.6 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® ENH4565 PBT (Asia Pacific)
33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE.
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
10.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® ENH4565 PBT (Asia Pacific)
33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE.
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
10.6 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Valox® ENH4565 PBT (Asia Pacific)
33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE.
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
10.6 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® ENH4565 PBT (Europe-Africa-Middle East)
33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE.
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
10.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® ENH4565 PBT (Europe-Africa-Middle East)
33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE.
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
10.6 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Valox® ENH4565 PBT (Europe-Africa-Middle East)
33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE.
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
10.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® ENH8560 PBT+PET (Europe-Africa-Middle East)
Non-Brominated & Non-Chlorinated Flame Retardant, 30% Glass fiber reinforced PBT/PET blend
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
10.6 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Stat-kon EE005 PEI (Asia Pacific)
LNP STAT-KON* EE005 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the ..
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
10.6 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON EE005E PEI
LNP STAT-KON* EE005E is a compound based on Polyetherimide resin containing 25% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive.
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
10.6 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON EE005E PEI (Asia Pacific)
LNP STAT-KON* EE005E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
10.6 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP EC005 PEI
LNP THERMOCOMP* EC005 is a compound based on Polyetherimide resin containing 25% Carbon Fiber. Added features of this material include: Electrically Conductive.
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
10.6 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP EC005 PEI (Asia Pacific)
LNP THERMOCOMP* EC005 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
10.6 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Thermocomp OFJ66 PPS - Linear
LNP* Thermocomp* OFJ66 is a compound based on PPS - Linear resin containing Glass Fiber, Mineral. Added features of this material include: Low Warpage.This data was supplied by SABIC-IP for the Ame..
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
10.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp OFJ66 PPS - Linear
LNP* Thermocomp* OFJ66 is a compound based on PPS - Linear resin containing Glass Fiber, Mineral. Added features of this material include: Low Warpage.This data was supplied by SABIC-IP for the Ame..
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
10.6 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® EXVX1403 PBT (Asia Pacific)
33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE.
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
10.6 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Valox® EXVX1403 PBT (Asia Pacific)
33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE.
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
10.6 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® IQNH4565 PBT (Asia Pacific)
Valox* iQNH4565 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 29% based on EPEAT..
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
10.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® IQNH4565 PBT (Asia Pacific)
Valox* iQNH4565 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 29% based on EPEAT..
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
10.6 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Valox® IQNH4565 PBT (Asia Pacific)
Valox* iQNH4565 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 29% based on EPEAT..
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
10.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp OFJ66 PPS - Linear (Asia Pacific)
LNP* Thermocomp* OFJ66 is a compound based on PPS - Linear resin containing Glass Fiber, Mineral. Added features of this material include: Low Warpage.This data was supplied by SABIC-IP for the Asi..
Copyright © lookpolymers.com All Rights Reserved