Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 980 °C | 1800 °F | |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; HT (TH04) Temper; over 51 to 76 mm Thickness (UNS C17000) Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Liquidus | 980 °C | 1800 °F | |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; HT (TH04) Temper; up to 9.5 mm Thickness (UNS C17000) Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Liquidus | 980 °C | 1800 °F | |
Materion Beryllium Copper Alloy 165 Rod and Bar; A (TB00) Temper; All Sizes (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Liquidus | 980 °C | 1800 °F | |
Materion Beryllium Copper Alloy 165 Rod and Bar; AT (TF00) Temper; up to 76 mm (UNS C17000) Treatment required for max strength: 3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material.. |
|||
Liquidus | 980 °C | 1800 °F | |
Materion Beryllium Copper Alloy 165 Rod and Bar; H (TD04) Temper; up to 9.5 mm (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Liquidus | 980 °C | 1800 °F | |
Materion Beryllium Copper Alloy 190 Strip; AM (TM00) Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 67%Formability Ratio, 90° Bend, R.. |
|||
Liquidus | 980 °C | 1800 °F | |
Materion Beryllium Copper Alloy 190 Strip; XHMS (TM08) Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%Stress Relaxation after 1000 hrs @ 200°C: 69%Formability Ratio, 90° Bend, R.. |
|||
Liquidus | 980 °C | 1800 °F | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; A (TB00) Temper; All Thicknesses (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Liquidus | 980 °C | 1800 °F | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; H (TD04) Temper; over 51 to 76 mm Thickness (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Liquidus | 980 °C | 1800 °F | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; HT (TH04) Temper; over 25 to 51 mm Thickness (UNS C17200) Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Liquidus | 980 °C | 1800 °F | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; HT (TH04) Temper; over 51 to 76 mm Thickness (UNS C17200) Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Liquidus | 980 °C | 1800 °F | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; HT (TH04) Temper; over 9.5 to 25 mm Thickness (UNS C17200) Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Liquidus | 980 °C | 1800 °F | |
Materion Beryllium Copper Alloy 25 Rod and Bar; A (TB00) Temper; All Sizes (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Liquidus | 980 °C | 1800 °F | |
Materion Beryllium Copper Alloy 25 Rod and Bar; H (TD04) Temper; over 25.4 to 76 mm (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Liquidus | 980 °C | 1800 °F | |
Materion Beryllium Copper Alloy 25 Rod and Bar; H (TD04) Temper; over 9.5 to 25.4 mm (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Liquidus | 980 °C | 1800 °F | |
Materion Beryllium Copper Alloy 25 Rod and Bar; HT (TH04) Temper; up to 9.5 mm (UNS C17200) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Liquidus | 980 °C | 1800 °F | |
Materion Beryllium Copper Alloy 25 Strip; A -Planished (TB00) Temper (UNS C17200) Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0Formability Ratio (bad Way): 0Superficial Hardness: 30T 46-67Tabulated properties apply .. |
|||
Liquidus | 980 °C | 1800 °F | |
Materion Beryllium Copper Alloy 25 Strip; H (TD04) Temper (UNS C17200) Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 1Formability Ratio (bad Way): 2.9Superficial Hardness: 30T 79-83Tabulated properties appl.. |
|||
Liquidus | 980 °C | 1800 °F | |
Materion Beryllium Copper Alloy 25 Wire; 1/4HT (TH01) Temper; 1.3-12.7 mm Diameter (UNS C17200) Treatment required for max strength: 2 hrs @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed i.. |
|||
Liquidus | 980 °C | 1800 °F | |
Materion Beryllium Copper Alloy 25 Wire; AT (TF00) Temper; 1.3-12.7 mm Diameter (UNS C17200) Treatment required for max strength: 3 hrs @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed i.. |
|||
Liquidus | 980 °C | 1800 °F | |
Materion Beryllium Copper Alloy 25 Wire; HT (TH04) Temper; 1.3-2.0 mm Diameter (UNS C17200) Treatment required for max strength: 1 hr @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed it.. |
|||
Liquidus | 980 °C | 1800 °F | |
Materion Beryllium Copper Alloy M25 Rod and Bar; AT (TF00) Temper; up to 76 mm (UNS C17300) Treatment required for max strength: 3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material.. |
|||
Liquidus | 980 °C | 1800 °F | |
Materion Beryllium Copper Alloy M25 Rod and Bar; HT (TH04) Temper; over 25.4 to 76 mm (UNS C17300) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Liquidus | 980 °C | 1800 °F | |
Materion Beryllium Copper Alloy M25 Wire; 1/2HT (TH02) Temper; 1.3-12.7 mm Diameter (UNS C17300) Treatment required for max strength: 1.5 hrs @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed.. |
|||
Liquidus | 980 °C | 1800 °F | |
Materion Brushform® 290 Beryllium Copper Alloy Strip; TM08 Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation after 1000 hrs @ 200°C: 78%Formability Ratio, 90° Bend, R.. |
|||
Liquidus | 980 °C | 1800 °F | |
Materion Beryllium Copper Alloy M25 Wire; H (TD04) Temper; 1.3-2.0 mm Diameter (UNS C17300) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Liquidus | 980 °C | 1800 °F | |
CMW® D158F Silver Graphite Contact Material For electrical contacts; reduced sticking, low frictionInformation provided by CMW Inc. |
|||
Liquidus | 980 °C | 1800 °F | |
CMW® D355F Pre-oxidized Silver Cadmium Oxide Contact Material ASTM B781 Table 3 For electrical contacts; resistant to welding and high surge currentsInformation provided by CMW Inc. |
|||
Liquidus | 980 °C | 1800 °F | |
CMW® D54F Pre-oxidized Silver Cadmium Oxide Contact Material ASTM B781, Table 3 For electrical contacts; resistant to welding and high surge currentsInformation provided by CMW Inc. |
|||
Liquidus | 980 °C | 1800 °F | |
CMW® D55X Post-oxidized Silver Cadmium Oxide Contact Material ASTM B781, Table 3 For electrical contacts; resistant to welding and high surge currentsInformation provided by CMW Inc. |