Thermal Properties Metric English Comments
Solidus 1301 °C
2374 °F
Haynes 230® alloy plate
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Solidus 1301 °C
2374 °F
Haynes 230® alloy plate, 1000 hours exposure at 649°C (1200°F)
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Solidus 1301 °C
2374 °F
Haynes 230® alloy plate, 4000 hours exposure at 649°C (1200°F)
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Solidus 1301 °C
2374 °F
Haynes 230® alloy, 0% cold reduction
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Solidus 1301 °C
2374 °F
Haynes 230® alloy, 10% cold reduction
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Solidus 1301 °C
2374 °F
Haynes 230® alloy, 10% cold reduction, 1066°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Solidus 1301 °C
2374 °F
Haynes 230® alloy, 10% cold reduction, 1177°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Solidus 1301 °C
2374 °F
Haynes 230® alloy, 20% cold reduction, 1066°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Solidus 1301 °C
2374 °F
Haynes 230® alloy, 20% cold reduction, 1121°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Solidus 1301 °C
2374 °F
Haynes 230® alloy, 20% cold reduction, 1177°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Solidus 1301 °C
2374 °F
Haynes 230® alloy, 30% cold reduction
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Solidus 1301 °C
2374 °F
Haynes 230® alloy, 30% cold reduction, 1066°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Solidus 1301 °C
2374 °F
Haynes 230® alloy, 30% cold reduction, 1121°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Solidus 1301 °C
2374 °F
Haynes 230® alloy, 30% cold reduction, 1177°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Solidus 1301 °C
2374 °F
Haynes 230® alloy, 40% cold reduction
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Solidus 1301 °C
2374 °F
Haynes 230® alloy, 40% cold reduction, 1066°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Solidus 1301 °C
2374 °F
Haynes 230® alloy, 40% cold reduction, 1121°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Solidus 1301 °C
2374 °F
Haynes 230® alloy, 40% cold reduction, 1177°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Solidus 1301 °C
2374 °F
Haynes 230® alloy, plate, 1000 hours exposure at 871°C (1600°F)
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Solidus 1301 °C
2374 °F
Haynes 230® alloy, plate, 4000 hours exposure at 760°C (1400°F)
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Solidus 1301 °C
2374 °F
Haynes 230® alloy, plate, 8000 hours exposure at 760°C (1400°F)
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Solidus 1301 °C
2374 °F
Haynes 230® alloy, plate, 8000 hours exposure at 871°C (1600°F)
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Solidus 1301 °C
2374 °F
Special Metals INCONEL® 601GC® Nickel Superalloy
Data provided by the manufacturer, Special Metals.
Solidus 1301 °C
2374 °F
Haynes 230® alloy, GMAW deposit weld metal
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..
Solidus 1301 °C
2374 °F
Haynes 230® alloy, plate, 16000 hours exposure at 760°C (1400°F)
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..
Solidus 1301 °C
2374 °F
Haynes 230® alloy, plate, 16000 hours exposure at 871°C (1600°F)
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..
Solidus 1301 °C
2374 °F
Haynes 230® alloy, 50% cold reduction
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..
Solidus 1301 °C
2374 °F
Haynes 230® alloy, 50% cold reduction, 1066°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..
Solidus 1301 °C
2374 °F
Haynes 230® alloy, 50% cold reduction, 1121°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..
Solidus 1301 °C
2374 °F
Haynes 230® alloy, plate, 4000 hours exposure at 871°C (1600°F)
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..