Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.510 - 0.610 W/m-K @Temperature 600 °C |
3.54 - 4.23 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 110 C AL Dense Refractory Castable Description: Because of special addition this coarse castable shows a very good resistance against liquid aluminum metal.Remarks: These values apply to cast products.Information provided by Gouda Vu.. |
|||
Thermal Conductivity | 0.510 - 0.610 W/m-K @Temperature 600 °C |
3.54 - 4.23 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 120 Dense Refractory Castable Description: A general purpose castable for use up to 1200°C under normal operating conditions. Curon 120 has good thermal shock resistance.Remarks: These values apply to cast products. Also avai.. |
|||
Thermal Conductivity | 0.510 - 0.610 W/m-K @Temperature 600 °C |
3.54 - 4.23 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 120 HS Dense Refractory Castable Description: This castable has a very good resistance against thermal shocks because of its low thermal expansion. In addition, it has a high strength. Used in incinerators and for tunnel kiln cars... |
|||
Thermal Conductivity | 0.510 - 0.610 W/m-K @Temperature 100 °C |
3.54 - 4.23 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 130 Dense Refractory Castable Description: Curon 130 is a castable with a good workability and a high strength. Therefore this castable can be characterized as a reliable refractory construction material.Remarks: These values ap.. |
|||
Thermal Conductivity | 0.510 - 0.610 W/m-K @Temperature 100 °C |
3.54 - 4.23 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 140 Dense Refractory Castable Description: Because of its relatively low Fe2O3 content and its high alumina percentages, this castable can be applied up to 1400°C in slightly reducing atmospheres. Up to high temperatures Curo.. |
|||
Thermal Conductivity | 0.510 - 0.610 W/m-K @Temperature 100 °C |
3.54 - 4.23 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 150 HS Dense Refractory Castable Description: Dense refractory castableRemarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information provided by Gouda Vuurvast. |
|||
Thermal Conductivity | 0.410 - 0.610 W/m-K @Temperature 600 °C |
2.85 - 4.23 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast FI 55-11 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Thermal Conductivity | 0.510 - 0.610 W/m-K @Temperature 1400 °C |
3.54 - 4.23 BTU-in/hr-ft²-°F @Temperature 2550 °F |
|
Gouda Vuurvast GOLITE 160 Refractory Insulating Castable Description: This castable can be used up to very high temperatures under reducing conditions.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information.. |
|||
Thermal Conductivity | 0.510 - 0.610 W/m-K @Temperature 600 °C |
3.54 - 4.23 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 130 HRC AL Dense Refractory Castable Description: Because of special addition this castable is used for the walls above the liquid level in aluminum melting furnaces.Remarks: These values apply to cast products.Information provided by .. |
|||
Thermal Conductivity | 0.510 - 0.610 W/m-K @Temperature 600 °C |
3.54 - 4.23 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 130 HRC Dense Refractory Castable Description: A coarse, low iron castable for use up to 1300°C under normal operation conditions, also usable under reducing circumstances. Curon 130 HRC has a good thermal shock resistance becaus.. |
|||
Thermal Conductivity | 0.510 - 0.610 W/m-K @Temperature 600 °C |
3.54 - 4.23 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 130 HRCC RAPID Dense Refractory Castable Description: An extra coarse, low iron castable for use to 1300°C under normal operation conditions, also usable under reducing circumstances. Curon 130 HRCC RAPID has good thermal shock resistan.. |