Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.35 W/m-K @Temperature 1100 °C |
9.37 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast B Sp Dense Refractory Brick Description: A very dense brick, high resistance against slag penetration. Application: in rotary kilns (cement) and incinerators.Remarks: This data represents average values, obtained from samples .. |
|||
Thermal Conductivity | 1.35 - 1.55 W/m-K @Temperature 100 °C |
9.37 - 10.8 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURAS PBK D Moldable Refractory Material Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. This moldable contains a phosphate binding agent and has a low silica cont.. |
|||
Thermal Conductivity | 1.35 - 1.55 W/m-K @Temperature 100 °C |
9.37 - 10.8 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURAS PBK DGM Moldable Refractory Material Description: This material is supplied as a dry gunning powder. This moldable contains a phosphate binding agent and has a low silica content. For a large variety of applications this results in goo.. |
|||
Thermal Conductivity | 1.35 - 1.45 W/m-K @Temperature 100 °C |
9.37 - 10.1 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 170 Dense Refractory Castable Description: A general purpose castable with a wide range of applications for high temperatures. The low Fe2O3 content makes this castable suitable for use under reducing conditions.Remarks: These v.. |
|||
Thermal Conductivity | 1.35 - 1.45 W/m-K @Temperature 100 °C |
9.37 - 10.1 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 170 GM Dense Refractory Castable Description: A general purpose gunning castable with a wide range of applications for high temperatures. The low Fe2O3 content makes this castable suitable for use under reducing conditions.Remarks:.. |
|||
Thermal Conductivity | 1.35 - 1.55 W/m-K @Temperature 1600 °C |
9.37 - 10.8 BTU-in/hr-ft²-°F @Temperature 2910 °F |
|
Gouda Vuurvast CURON 180 B Dense Refractory Castable Description: This high quality castable is marked by a high refractoriness and a good thermal shock resistance. Because it has a high alumina content and a low percentage of Fe2O3, this castable can.. |
|||
Thermal Conductivity | 1.35 - 1.55 W/m-K @Temperature 1600 °C |
9.37 - 10.8 BTU-in/hr-ft²-°F @Temperature 2910 °F |
|
Gouda Vuurvast CURON 180 Dense Refractory Castable Description: This high quality, corundum based castable is marked by a high refractoriness and a good thermal shock resistance. Because it has a high alumina content and a low percentage of SiO2, th.. |
|||
Thermal Conductivity | 1.35 - 1.55 W/m-K @Temperature 1600 °C |
9.37 - 10.8 BTU-in/hr-ft²-°F @Temperature 2910 °F |
|
Gouda Vuurvast CURON 180 TF Dense Refractory Castable Description: Curon 180 TF is a tabular alumina based castable, highly abrasion resistant, especially developed for application in the vacuum ladle treatment installation in the steel refinery.Remark.. |
|||
Thermal Conductivity | 1.35 - 1.45 W/m-K @Temperature 600 °C |
9.37 - 10.1 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast VIBRON 160 H GS (R) Dense Vibrating Refractory Castable Description: Vibron 160 H GS (R) is a pumpable low cement castable based on high fired high alumina grog and characterized by a high strength and good thermal shock-, corrosion- and abrasion resista.. |
|||
Thermal Conductivity | 1.35 - 1.55 W/m-K @Temperature 100 °C |
9.37 - 10.8 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast VIBRON 160 H SiC Dense Vibrating Refractory Castable Description: Vibron 160 H SiC is a low cement vibrating castable characterized by a high strength, good abrasion resistance and excellent thermal shock resistance. Because of the presence of SiC, th.. |
|||
Thermal Conductivity | 1.35 - 1.55 W/m-K @Temperature 100 °C |
9.37 - 10.8 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURAS PBK Moldable Refractory Material Description: This moldable contains a phosphate binding agent and has a low silica content. For a large variety of applications this results in a good slag resistance and high strength properties at.. |
|||
Thermal Conductivity | 1.35 W/m-K @Temperature 800 °C, Time 10800 sec |
9.37 BTU-in/hr-ft²-°F @Temperature 1470 °F, Time 3.00 hour |
|
Sharadaa Ceramics REFCAST LC45 Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Thermal Conductivity | 1.35 - 1.55 W/m-K @Temperature 1600 °C |
9.37 - 10.8 BTU-in/hr-ft²-°F @Temperature 2910 °F |
|
Gouda Vuurvast CURON 180 T Sp Dense Refractory Castable Description: Curon 180 T special is a tabular alumina based castable, highly resistant against abrasion, dust erosion or heavy impact even at extremely high temperatures.Remarks: These values apply .. |