Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.28 - 1.48 W/m-K @Temperature 600 °C |
8.88 - 10.3 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 180 B Dense Refractory Castable Description: This high quality castable is marked by a high refractoriness and a good thermal shock resistance. Because it has a high alumina content and a low percentage of Fe2O3, this castable can.. |
|||
Thermal Conductivity | 1.28 - 1.48 W/m-K @Temperature 600 °C |
8.88 - 10.3 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 180 Dense Refractory Castable Description: This high quality, corundum based castable is marked by a high refractoriness and a good thermal shock resistance. Because it has a high alumina content and a low percentage of SiO2, th.. |
|||
Thermal Conductivity | 1.28 - 1.48 W/m-K @Temperature 600 °C |
8.88 - 10.3 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 180 TF Dense Refractory Castable Description: Curon 180 TF is a tabular alumina based castable, highly abrasion resistant, especially developed for application in the vacuum ladle treatment installation in the steel refinery.Remark.. |
|||
Thermal Conductivity | 1.28 - 1.38 W/m-K @Temperature 600 °C |
8.88 - 9.58 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast VIBRON 170 M Dense Vibrating Refractory Castable Description: Vibron 170 is a low cement castable based on synthetic mullite grog and is characterized by a high strength, excellent thermal shock resistance and high resistance to liquid slags.Remar.. |
|||
Thermal Conductivity | 1.28 - 1.38 W/m-K @Temperature 600 °C |
8.88 - 9.58 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast VIBRON 170 M GS (R) Dense Vibrating Refractory Castable Description: Vibron 170 M GS (R) is a low cement castable based on synthetic mullite grog and is characterized by a high strength, excellent thermal shock resistance and high resistance to liquid sl.. |
|||
Thermal Conductivity | 1.28 - 1.38 W/m-K @Temperature 600 °C |
8.88 - 9.58 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast VIBRON 170 M RAPID Dense Vibrating Refractory Castable Description: Vibron 170 M Rapid is a low cement castable based on synthetic mullite grog and is characterized by a high strength, excellent thermal shock resistance and high resistance to liquid sla.. |
|||
Thermal Conductivity | 1.28 W/m-K @Temperature 600 °C, Time 10800 sec |
8.88 BTU-in/hr-ft²-°F @Temperature 1110 °F, Time 3.00 hour |
|
Sharadaa Ceramics REFCAST 80 High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Thermal Conductivity | 1.28 W/m-K @Temperature 400 °C, Time 10800 sec |
8.88 BTU-in/hr-ft²-°F @Temperature 752 °F, Time 3.00 hour |
|
Sharadaa Ceramics REFCAST A High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Thermal Conductivity | 1.28 W/m-K @Temperature 600 °C, Time 10800 sec |
8.88 BTU-in/hr-ft²-°F @Temperature 1110 °F, Time 3.00 hour |
|
Sharadaa Ceramics REFCAST LC60 Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Thermal Conductivity | 1.28 W/m-K @Temperature 800 °C, Time 10800 sec |
8.88 BTU-in/hr-ft²-°F @Temperature 1470 °F, Time 3.00 hour |
|
Sharadaa Ceramics REFCAST LC60ABR Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Thermal Conductivity | 1.28 - 1.48 W/m-K @Temperature 600 °C |
8.88 - 10.3 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 180 T Sp Dense Refractory Castable Description: Curon 180 T special is a tabular alumina based castable, highly resistant against abrasion, dust erosion or heavy impact even at extremely high temperatures.Remarks: These values apply .. |
|||
Thermal Conductivity | 1.28 - 1.48 W/m-K @Temperature 1600 °C |
8.88 - 10.3 BTU-in/hr-ft²-°F @Temperature 2910 °F |
|
Gouda Vuurvast CURON 185 T Dense Refractory Castable Description: Curon 185 T is a very pure high alumina castable based on tabular alumina with very low Fe2O3 and SiO2 contents. Suitable for use in strongly reducing atmospheres.Remarks: These values .. |