Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.16 - 1.26 W/m-K @Temperature 1000 °C |
8.05 - 8.74 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Gouda Vuurvast CURON 160 FS Dense Refractory Castable Description: This castable is based on fused silica. It has an extremely good thermal shock resistance and minor expansion behavior up to process temperature of 900°C. Application: zinc melting f.. |
|||
Thermal Conductivity | 1.16 W/m-K @Temperature 400 °C, Time 10800 sec |
8.05 BTU-in/hr-ft²-°F @Temperature 752 °F, Time 3.00 hour |
|
Sharadaa Ceramics REFCAST HA High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Thermal Conductivity | 1.16 W/m-K @Temperature 600 °C, Time 10800 sec |
8.05 BTU-in/hr-ft²-°F @Temperature 1110 °F, Time 3.00 hour |
|
Sharadaa Ceramics REFCAST LC60ABR Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Thermal Conductivity | 1.16 W/m-K @Temperature 400 °C, Time 10800 sec |
8.05 BTU-in/hr-ft²-°F @Temperature 752 °F, Time 3.00 hour |
|
Sharadaa Ceramics REFCAST HA PLUS High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |