Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.470 W/m-K @Temperature 686 °C |
3.26 BTU-in/hr-ft²-°F @Temperature 1270 °F |
hot face 842°C, cold face 529°C, mean - 686°C |
Pyrotek Insural® 140 Insulating Refractory Shapes for Aluminum Insural® 140 Precast Shapes are designed for the containment of molten aluminum in hot top modules (cross feeder) and trough/launder applications.AdvantagesNear zero expansion avoids gaps at the jo.. |
|||
Thermal Conductivity | 0.470 W/m-K @Temperature 200 °C |
3.26 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Pyrotek NAD-11 Structural Insulation Board NAD-11 is an asbestos-free cement board with excellent electrical properties. It has a high density cement board reinforced with inorganic fibers.ApplicationsCathode support pads Platen insulation .. |
|||
Thermal Conductivity | 0.470 W/m-K @Temperature 100 °C |
3.26 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E1530 |
3M Dyneon™ CC646/S Custom Compound
(discontinued **) This compound consists of a mixture of 60% bronze blended with PTFE.Information provided by Dyneon, A 3M Company |
|||
Thermal Conductivity | 0.470 - 0.570 W/m-K @Temperature 100 °C |
3.26 - 3.96 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 110 C AL Dense Refractory Castable Description: Because of special addition this coarse castable shows a very good resistance against liquid aluminum metal.Remarks: These values apply to cast products.Information provided by Gouda Vu.. |
|||
Thermal Conductivity | 0.470 - 0.570 W/m-K @Temperature 100 °C |
3.26 - 3.96 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 120 Dense Refractory Castable Description: A general purpose castable for use up to 1200°C under normal operating conditions. Curon 120 has good thermal shock resistance.Remarks: These values apply to cast products. Also avai.. |
|||
Thermal Conductivity | 0.470 - 0.570 W/m-K @Temperature 100 °C |
3.26 - 3.96 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 120 HS Dense Refractory Castable Description: This castable has a very good resistance against thermal shocks because of its low thermal expansion. In addition, it has a high strength. Used in incinerators and for tunnel kiln cars... |
|||
Thermal Conductivity | 0.470 - 0.570 W/m-K @Temperature 1000 °C |
3.26 - 3.96 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Gouda Vuurvast FI 45-12 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Thermal Conductivity | 0.470 - 0.570 W/m-K @Temperature 1260 °C |
3.26 - 3.96 BTU-in/hr-ft²-°F @Temperature 2300 °F |
|
Gouda Vuurvast GOLITE 145 Refractory Insulating Castable Description: Golite 145 can be used in direct contact with the furnace conditions and combines a high strength with a good thermal insulation.Remarks: These values apply to cast products. Also avail.. |
|||
Thermal Conductivity | 0.470 - 0.570 W/m-K @Temperature 1370 °C |
3.26 - 3.96 BTU-in/hr-ft²-°F @Temperature 2500 °F |
|
Gouda Vuurvast GOLITE 155 Refractory Insulating Castable Description: Due to it's high strength at high temperatures, this material can be applied in direct contact with the firing process.Remarks: These values apply to cast products. Also available i.. |
|||
Thermal Conductivity | 0.470 - 0.570 W/m-K @Temperature 100 °C |
3.26 - 3.96 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 130 HRC AL Dense Refractory Castable Description: Because of special addition this castable is used for the walls above the liquid level in aluminum melting furnaces.Remarks: These values apply to cast products.Information provided by .. |
|||
Thermal Conductivity | 0.470 - 0.570 W/m-K @Temperature 100 °C |
3.26 - 3.96 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 130 HRC Dense Refractory Castable Description: A coarse, low iron castable for use up to 1300°C under normal operation conditions, also usable under reducing circumstances. Curon 130 HRC has a good thermal shock resistance becaus.. |
|||
Thermal Conductivity | 0.470 - 0.570 W/m-K @Temperature 100 °C |
3.26 - 3.96 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 130 HRCC RAPID Dense Refractory Castable Description: An extra coarse, low iron castable for use to 1300°C under normal operation conditions, also usable under reducing circumstances. Curon 130 HRCC RAPID has good thermal shock resistan.. |