Pyrotek Pyrocast 80 Lightweight Castable Refractory
Pyrocast 80 is a lightweight, low cement, fused silica castable designed for moderate flow molten aluminum contact applications. Pyrocast 80 offers low thermal conductivity, excellent resistance to..
Thermal Conductivity 0.390 W/m-K

@Temperature 250 °C
2.71 BTU-in/hr-ft²-°F

@Temperature 482 °F
ASTM E1530
3M Dyneon™ CC655 PTFE, 50% Stainless Steel Filled  (discontinued **)
Type II, free flowing.Typical Applications: Finished or semi-finished parts: sheets, rods, tubes, billets for skiving of films or machining into complex shapes.Information provided by the Dyneon div..
Thermal Conductivity 0.390 W/m-K

@Temperature 100 °C
2.71 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1530
3M Dyneon™ CC622 PTFE 10% Graphite Filled  (discontinued **)
Product Form: Black, pelletized free-flowing powder. Applications include bearings, ring seals.Data provided by Dyneon.
Thermal Conductivity 0.390 W/m-K

@Temperature 250 °C
2.71 BTU-in/hr-ft²-°F

@Temperature 482 °F
ASTM E1530
3M Dyneon™ CC622 PTFE 10% Graphite Filled  (discontinued **)
Product Form: Black, pelletized free-flowing powder. Applications include bearings, ring seals.Data provided by Dyneon.
Thermal Conductivity 0.390 W/m-K

@Temperature 250 °C
2.71 BTU-in/hr-ft²-°F

@Temperature 482 °F
ASTM E1530
3M Dyneon™ CC646/S Custom Compound  (discontinued **)
This compound consists of a mixture of 60% bronze blended with PTFE.Information provided by Dyneon, A 3M Company
Thermal Conductivity 0.390 W/m-K

@Temperature 1400 °C
2.71 BTU-in/hr-ft²-°F

@Temperature 2550 °F
Parallel to Thickness; ASTM C177-76
Zircar Ceramics SALI Alumina Insulation
SALI has been serving 1700°C low mass furnace users longer than any other alumina fiber board available today. SALI is a premium grade rigid fiber board with superior hot strength.Information provi..
Thermal Conductivity 0.390 W/m-K

@Temperature 1350 °C
2.71 BTU-in/hr-ft²-°F

@Temperature 2460 °F
Parallel to Thickness; ASTM C177-76
Zircar Ceramics SALI-2 Alumina Insulation
SALI-2 is a premium grade rigid insulation board used as hotface insulation or a precision machined furnace fixtures.Information provided by Zircar Ceramics.
Thermal Conductivity 0.390 W/m-K

@Temperature 1093 °C
2.71 BTU-in/hr-ft²-°F

@Temperature 1999 °F
ASTM C182
BNZ Materials BNZ-28 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.390 W/m-K

@Temperature 1000 °C
2.71 BTU-in/hr-ft²-°F

@Temperature 1830 °F
ASTM C182
BNZ Materials BNZP-26 Insulating Firebrick (French Grade)
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.390 W/m-K

@Temperature 816 °C
2.71 BTU-in/hr-ft²-°F

@Temperature 1500 °F
ASTM C182
BNZ Materials PA 26 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.390 W/m-K

@Temperature 250 °C
2.71 BTU-in/hr-ft²-°F

@Temperature 482 °F
ASTM E1530
3M Dyneon™ CC085 Custom Fluoropolymer Compound  (discontinued **)
This compound consists of a mixture of PPS and other proprietary fillers blended with PTFE.Information provided by Dyneon, A 3M Company
Thermal Conductivity 0.390 - 0.490 W/m-K

@Temperature 600 °C
2.71 - 3.40 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast FI 35-12 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.