Polymer Property : Thermal Conductivity = 192 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 27.6 W/m-K

@Temperature 25.0 °C
192 BTU-in/hr-ft²-°F

@Temperature 77.0 °F
International Mold Steel DH21 Die Cast & Forging Steel
DH21 is for aluminum die cast dies.Information provided by International Mold Steel
Thermal Conductivity 27.6 W/m-K

@Temperature 700 °C
192 BTU-in/hr-ft²-°F

@Temperature 1290 °F
International Mold Steel DHA-World Die Cast & Forging Steel
DHA-World is a high hardenability and high tough general use hot work die steel.Information provided by International Mold Steel
Thermal Conductivity 27.7 W/m-K

@Temperature 315 °C
192 BTU-in/hr-ft²-°F

@Temperature 599 °F
Crucible Steel Nu-Die® V (AISI H13) Hot Work Tool Steel
Nu-Die® V (AISI H13) has been the most popular, and perhaps the most versatile hot work tool steel available for many years. It provides a good balance of toughness, heat check resistance and tempe..
Thermal Conductivity 27.7 W/m-K

@Temperature 315 °C
192 BTU-in/hr-ft²-°F

@Temperature 599 °F
Crucible Steel Nu-Die® XL (Premium Quality AISI H13) Tool Steel
Nu-Die XL (AISI H13) is a premium version of H13 tool steel manufactured, tested and certified to meet stringent die casting industry specifications issued by NADCA, Chrysler and others. It offers b..
Thermal Conductivity 27.6 W/m-K

@Temperature 800 °C
192 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Assab Steels 8407 2M Hot Work Steel
ASSAB 8407 is a chromium-molybdenum-vanadium-alloyed steel which is characterized by: Good resistance to abrasion at both low and high temperatures. High level of toughness and ductility Uniform ..
Thermal Conductivity 27.7 W/m-K

@Temperature 500 °C
192 BTU-in/hr-ft²-°F

@Temperature 932 °F
Hardened and Tempered
Bohler-Uddeholm BÖHLER W302 ISOBLOC® H13 hot work tool steel
Properties:Hot work tool steel featuring excellent hot tensile properties, high hot wear resistance, adequate toughness and heat checking resistance, adequate toughness and heat checking; admits wat..
Thermal Conductivity 27.6 W/m-K

@Temperature 800 °C
192 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Assab Steels 8407 SUPREME Hot Work Steel
8407 SUPREME is characterized by:High level of resistance to thermal shock and thermal fatigueGood high temperature strengthExcellent toughness and ductility in all directionsGood machinability and ..
Thermal Conductivity 27.7 W/m-K

@Temperature 100 °C
192 BTU-in/hr-ft²-°F

@Temperature 212 °F
Quenched and Tempered
Schmolz + Bickenbach Cryodur® 2767 Cold Work Die Steel
Description: High hardenability and toughness, highly suitable for polishing, texturing and EDM machining. We recommend the use of Cryodur® 2767 (ERS) for extreme demandsApplications: Cutlery dies,..