Thermal Properties Metric English Comments
Thermal Conductivity 2.20 W/m-K

@Temperature 100 °C
15.3 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast AC 80-10 Dense Refractory Brick
Description: This bauxite base brick shows, due to the addition of CR2O3, a very good slag resistance.Remarks: This data represents average values, obtained from samples that were cut from standard ..
Thermal Conductivity 2.20 W/m-K

@Temperature 100 °C
15.3 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast AC 80-5 Dense Refractory Brick
Description: This Cr2O3 containing brick shows a good slag and abrasion resistance. Application in ZnO furnaces.Remarks: This data represents average values, obtained from samples that were cut from..
Thermal Conductivity 2.20 W/m-K

@Temperature 1100 °C
15.3 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Gouda Vuurvast AC 85-5 Dense Refractory Brick
Description: Excellent resistance against alkali- and metal slags. A good volume stability at very high temperatures. Application: chemical incinerators, combustion chambers for very high temperatur..
Thermal Conductivity 2.20 W/m-K

@Temperature 100 °C
15.3 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast AK 70 M Dense Refractory Brick
Description: This mullite brick is characterized by a very good thermal shock resistance, a high resistance against slag penetration and a high strength.Remarks: This data represents average values,..
Thermal Conductivity 2.20 W/m-K

@Temperature 1100 °C
15.3 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Gouda Vuurvast AK 80 FM Dense Refractory Brick
Description: This fused mullite based brick has a very good thermal shock resistance and an excellent resistance against liquid slags at high temperature.Remarks: This data represents average values..
Thermal Conductivity 2.20 W/m-K

@Temperature 1100 °C
15.3 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Gouda Vuurvast AK 90 Dense Refractory Brick
Description: This brick can be used in very severe conditions, i.e. in reducing atmosphere at a high temperatures, e.g. in carbon-black furnaces.Remarks: This data represents average values, obtaine..
Thermal Conductivity 2.20 W/m-K

@Temperature 1100 °C
15.3 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Gouda Vuurvast LP 80 A Dense Refractory Brick
Description: LP 80 is a low porosity brick based on sintered bauxite with an extremely high abrasion resistance and therefore very well suited for application in rotary cement furnaces.Remarks: This..
Thermal Conductivity 2.20 W/m-K

@Temperature 100 °C
15.3 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast AK 70 KP Dense Refractory Brick
Description: A high quality phosphate bonded andalusite/corundum brick with very good volume stability. Also good slag resistance and thermal shock resistance. Remarks: This data represents average ..
Thermal Conductivity 2.20 W/m-K

@Temperature 650 °C
15.3 BTU-in/hr-ft²-°F

@Temperature 1200 °F
Gouda Vuurvast AK 85 KM Dense Refractory Brick
Description: This brick based on mullite and corundum, is characterized by a very low porosity, high slag resistance, low creep and very good thermal shock resistance.Remarks: This data represents a..
Thermal Conductivity 2.20 - 4.20 W/m-K

@Temperature 1400 °C
15.3 - 29.1 BTU-in/hr-ft²-°F

@Temperature 2550 °F
Gouda Vuurvast VIBRON 160 K 50 Dense Vibrating Refractory Castable
Description: Vibron 160 K 50 is a low cement castable based on silicon carbide and characterized by a very good thermal conductivity, high abrasion resistance and a good oxidation resistance up to 1..
Thermal Conductivity 2.20 W/m-K

@Temperature 500 °C
15.3 BTU-in/hr-ft²-°F

@Temperature 932 °F
COI Ceramics Nicalon™ CG SiCO Ceramic Fiber
Description: The fiber is homogeneously composed of ultra-fine beta-SiC crystallites and an amorphous mixture of silicon, carbon, and oxygen. The fiber has excellent strength and modulus properties ..
Copyright © lookpolymers.com All Rights Reserved