Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.90 W/m-K @Temperature 23.0 °C |
13.2 BTU-in/hr-ft²-°F @Temperature 73.4 °F |
Along flow; ISO 22007-4 |
Victrex® PEEK 90HMF20 Polyetheretherketone (PEEK), 20% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 20% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, color black.T.. |
|||
Thermal Conductivity | 1.90 W/m-K @Temperature 1100 °C |
13.2 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast AC 80-10 Dense Refractory Brick Description: This bauxite base brick shows, due to the addition of CR2O3, a very good slag resistance.Remarks: This data represents average values, obtained from samples that were cut from standard .. |
|||
Thermal Conductivity | 1.90 W/m-K @Temperature 1100 °C |
13.2 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast AC 80-5 Dense Refractory Brick Description: This Cr2O3 containing brick shows a good slag and abrasion resistance. Application in ZnO furnaces.Remarks: This data represents average values, obtained from samples that were cut from.. |
|||
Thermal Conductivity | 1.90 W/m-K @Temperature 1100 °C |
13.2 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast AK 70 K Dense Refractory Brick Description: A high quality andalusite/corundum brick with a mullite bond with a very good volume stability. Also good slag- and thermal shock resistance.Remarks: This data represents average values.. |
|||
Thermal Conductivity | 1.90 W/m-K @Temperature 1100 °C |
13.2 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast AK 70 M Dense Refractory Brick Description: This mullite brick is characterized by a very good thermal shock resistance, a high resistance against slag penetration and a high strength.Remarks: This data represents average values,.. |
|||
Thermal Conductivity | 1.90 W/m-K @Temperature 650 °C |
13.2 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Gouda Vuurvast AK 80 FM Dense Refractory Brick Description: This fused mullite based brick has a very good thermal shock resistance and an excellent resistance against liquid slags at high temperature.Remarks: This data represents average values.. |
|||
Thermal Conductivity | 1.90 W/m-K @Temperature 100 °C |
13.2 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast LP 60 AAP Dense Refractory Brick Description: Special low porosity quality for use under severe corrosive conditions, (for instance liquid slags). Moreover, this brick has been extra protected against slag attack because it also co.. |
|||
Thermal Conductivity | 1.90 - 2.10 W/m-K @Temperature 1300 °C |
13.2 - 14.6 BTU-in/hr-ft²-°F @Temperature 2370 °F |
|
Gouda Vuurvast VIBRON 150 GZ (R) Dense Vibrating Refractory Castable Description: Vibron 150 GZ (R) is a low cement castable based on sintered South-American bauxite. The addition of zircon oxide in this product makes it suitable for areas under heavy chemical attack.. |
|||
Thermal Conductivity | 1.90 W/m-K @Temperature 1100 °C |
13.2 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast AK 70 A Dense Refractory Brick Description: This brick is made of a high quality bauxite. Application: transition zone of rotary cement kiln.Remarks: This data represents average values, obtained from samples that were cut from s.. |
|||
Thermal Conductivity | 1.90 W/m-K @Temperature 1100 °C |
13.2 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast AK 70 KP Dense Refractory Brick Description: A high quality phosphate bonded andalusite/corundum brick with very good volume stability. Also good slag resistance and thermal shock resistance. Remarks: This data represents average .. |
|||
Thermal Conductivity | 1.90 W/m-K @Temperature 300 °C |
13.2 BTU-in/hr-ft²-°F @Temperature 572 °F |
Warp direction |
COI Ceramics Sylramic™ S200 Silicon Carbide Ceramic Matrix Composite, CG Nicalon Engineered ceramic composite structure.Reinforcing Fiber Flexibility: S400 - Carbon Preceramic Polymer Matrix Precursors: S400 - Crystalline (SiC + Si3N4) or SiCPhysical Attributes: Dense Matrix ( |
|||
Thermal Conductivity | 1.90 W/m-K @Temperature 900 °C |
13.2 BTU-in/hr-ft²-°F @Temperature 1650 °F |
Thru-thickness |
COI Ceramics Sylramic™ S200 Silicon Carbide Ceramic Matrix Composite, CG Nicalon Engineered ceramic composite structure.Reinforcing Fiber Flexibility: S400 - Carbon Preceramic Polymer Matrix Precursors: S400 - Crystalline (SiC + Si3N4) or SiCPhysical Attributes: Dense Matrix ( |
|||
Thermal Conductivity | 1.90 W/m-K @Temperature 300 °C |
13.2 BTU-in/hr-ft²-°F @Temperature 572 °F |
Fill direction |
COI Ceramics Sylramic™ S200 Silicon Carbide Ceramic Matrix Composite, CG Nicalon Engineered ceramic composite structure.Reinforcing Fiber Flexibility: S400 - Carbon Preceramic Polymer Matrix Precursors: S400 - Crystalline (SiC + Si3N4) or SiCPhysical Attributes: Dense Matrix ( |
|||
Thermal Conductivity | 1.90 W/m-K @Temperature 100 °C |
13.2 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast LP 60 M Dense Refractory Brick Description: LP 60 M is a special low porosity, high strength material based on raw materials with a high mullite content. The grain distribution for these bricks is carefully selected, so that a ma.. |
|||
Thermal Conductivity | 1.90 W/m-K @Temperature 650 °C |
13.2 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Gouda Vuurvast LP 60 M Dense Refractory Brick Description: LP 60 M is a special low porosity, high strength material based on raw materials with a high mullite content. The grain distribution for these bricks is carefully selected, so that a ma.. |
|||
Thermal Conductivity | 1.90 - 2.10 W/m-K @Temperature 100 °C |
13.2 - 14.6 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast FLUCON 180 Dense Self Flowing Refractory Castable Description: Flucon 180 is a self flowing castable based on white fused Alumina. This castable is applied at severe thermal conditions and or severe slag attack.Remarks: These values apply to cast p.. |