Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 17.9 W/m-K @Temperature 400 °C |
124 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 538°C (1000°F), aged 16000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 17.9 W/m-K @Temperature 400 °C |
124 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 538°C (1000°F), aged 4000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 17.9 W/m-K @Temperature 400 °C |
124 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 538°C (1000°F), aged 8000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 17.9 W/m-K @Temperature 400 °C |
124 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 649°C (1200°F), aged 4000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 17.9 W/m-K @Temperature 400 °C |
124 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 760°C (1400°F), aged 16000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 17.9 W/m-K @Temperature 400 °C |
124 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 760°C (1400°F), aged 4000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 17.9 W/m-K @Temperature 400 °C |
124 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® S alloy, gas tungsten arc welded plate 12.7 mm (1/2 in.) thick Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 17.9 W/m-K @Temperature 400 °C |
124 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® S alloy, gas tungsten arc welded plate 12.7 mm (1/2 in.) thick, aged 1000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 17.9 W/m-K @Temperature 400 °C |
124 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® S alloy, gas tungsten arc welded plate 12.7 mm (1/2 in.) thick, aged 16000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 17.9 W/m-K @Temperature 400 °C |
124 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® S alloy, gas tungsten arc welded plate 12.7 mm (1/2 in.) thick, aged at 649°C (1200°F) for 8000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 17.9 W/m-K @Temperature 400 °C |
124 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® S alloy, gas tungsten arc welded, aged 1300 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 17.9 W/m-K @Temperature 400 °C |
124 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 427°C (800°F), aged 1000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 17.9 W/m-K @Temperature 400 °C |
124 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 427°C (800°F), aged 8000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 17.9 W/m-K @Temperature 400 °C |
124 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 871°C (1600°F), aged 8000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 17.9 W/m-K @Temperature 400 °C |
124 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® S alloy, weld metal, aged 16000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 17.9 W/m-K @Temperature 400 °C |
124 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® S alloy, weld metal, aged 4000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 17.9 W/m-K @Temperature 400 °C |
124 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® S alloy, weld metal, aged at 649°C (1200°F) for 1000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 17.8 W/m-K @Temperature 500 °C |
124 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Special Metals INCONEL® alloy 693 INCONEL alloy 693 is a new alloy from Special Metals which offers resistance to high temperature corrosion mechanisms not previously available from a nickel-based alloy. Of particular interest to t.. |
|||
Thermal Conductivity | 17.9 W/m-K @Temperature 149 °C |
124 BTU-in/hr-ft²-°F @Temperature 300 °F |
H900 |
Crucible Steel 15-5 Precipitation Hardening Stainless Steel Crucible 15-5 is a Premium Quality precipitation-hardening stainless steel which is capable of high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is a V.. |
|||
Thermal Conductivity | 17.9 W/m-K @Temperature 149 °C |
124 BTU-in/hr-ft²-°F @Temperature 300 °F |
H900 |
Crucible Steel 17Cr-4Ni Precipitation Hardening Stainless Steel Crucible 17Cr-4Ni is a precipitation-hardening stainless steel which is capable of a high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is martensitic a.. |
|||
Thermal Conductivity | 17.9 W/m-K @Temperature 149 °C |
124 BTU-in/hr-ft²-°F @Temperature 300 °F |
H900 |
Crucible Steel 17Cr-4Ni Super-X® Precipitation Hardening Stainless Steel Crucible 17Cr-4Ni is a version of 17CR-4Ni which has been modified to substantially improve machinability and other properties. Patented 17Cr-4Ni Super-X meets industry specifications for 17Cr-4Ni. .. |
|||
Thermal Conductivity | 17.9 W/m-K @Temperature 149 °C |
124 BTU-in/hr-ft²-°F @Temperature 300 °F |
|
AK Steel 15-5 PH® Precipitation Hardening Stainless Steel, Condition H 900 AK Steel 15-5 PH® provides high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base metal and welds. Short-time, .. |
|||
Thermal Conductivity | 17.9 W/m-K @Temperature 149 °C |
124 BTU-in/hr-ft²-°F @Temperature 300 °F |
condition H 900 |
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1100 (Heated 593°C) Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio.. |
|||
Thermal Conductivity | 17.9 W/m-K @Temperature 149 °C |
124 BTU-in/hr-ft²-°F @Temperature 300 °F |
condition H 900 |
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1075 (Heated 579°C) Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio.. |
|||
Thermal Conductivity | 17.9 W/m-K @Temperature 149 °C |
124 BTU-in/hr-ft²-°F @Temperature 300 °F |
condition H 900 |
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1150M (Heated 760°C/2hr/AC then 621°C/4hr/AC) Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio.. |
|||
Thermal Conductivity | 17.9 W/m-K @Temperature 149 °C |
124 BTU-in/hr-ft²-°F @Temperature 300 °F |
condition H 900 |
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 900 (Age-Hardened 482°C/1hr/AC) Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio.. |
|||
Thermal Conductivity | 17.9 W/m-K @Temperature 400 °C |
124 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 760°C (1400°F), aged 1000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Applications .. |
|||
Thermal Conductivity | 17.9 W/m-K @Temperature 400 °C |
124 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 871°C (1600°F), aged 4000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Applications .. |
|||
Thermal Conductivity | 17.9 W/m-K @Temperature 149 °C |
124 BTU-in/hr-ft²-°F @Temperature 300 °F |
condition H 900 |
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1025 (Heated 552°C) Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio.. |
|||
Thermal Conductivity | 17.9 W/m-K @Temperature 400 °C |
124 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Haynes Hastelloy® S alloy, gas tungsten arc welded plate 12.7 mm (1/2 in.) thick, aged 4000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Applications .. |