Thermal Properties Metric English Comments
Thermal Conductivity 0.700 - 0.800 W/m-K

@Temperature 100 °C
4.86 - 5.55 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURAS 50 PD Moldable Refractory Material
Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. Because of the addition of phosphate this type of moldable has a high stre..
Thermal Conductivity 0.600 - 0.800 W/m-K

@Temperature 1000 °C
4.16 - 5.55 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Gouda Vuurvast FI 25-15 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Thermal Conductivity 0.600 - 0.800 W/m-K

@Temperature 1000 °C
4.16 - 5.55 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Gouda Vuurvast FI 35-15 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Thermal Conductivity 0.600 - 0.800 W/m-K

@Temperature 1000 °C
4.16 - 5.55 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Gouda Vuurvast FI 45-15 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Thermal Conductivity 0.700 - 0.800 W/m-K

@Temperature 100 °C
4.86 - 5.55 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURAS 40 D Moldable Refractory Material
Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. Because of special additions this type of moldable has already a reasonabl..
Thermal Conductivity 0.700 - 0.800 W/m-K

@Temperature 100 °C
4.86 - 5.55 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURAS 40 PD Moldable Refractory Material
Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. Because of the addition of phosphate this type of moldable has a high stre..
Thermal Conductivity 0.700 - 0.800 W/m-K

@Temperature 100 °C
4.86 - 5.55 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURAS 50 D Moldable Refractory Material
Description: Because of special additions this moldable already has a reasonable strength at room temperature. This material is supplied as a dry powder, it has to be mixed with potable water to the..
Thermal Conductivity 0.700 - 0.800 W/m-K

@Temperature 600 °C
4.86 - 5.55 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURON 165 GM Dense Refractory Castable
Description: Curon 165 GM is based on bauxite and very pure chamotte grog. In has very good thermal shock resistance and a low firing shrinkage.Remarks: These values apply to cast products. Other mo..