Thermal Properties Metric English Comments
Thermal Conductivity 0.340 W/m-K

@Temperature 600 °C
2.36 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Pyrotek ISOMAG® 175 Structural Insulation Board
Isomag® 70 is a high strength insulating board suitable as an electrical insulator or a thermal barrier material in a variety of industrial applications. Its magnesia silicate based formulation pr..
Thermal Conductivity 0.340 W/m-K

@Temperature 100 °C
2.36 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1530
3M Dyneon™ CC503 PTFE, 15% Mineral Filled  (discontinued **)
Product Form: White, pelletized free-flowing powder. Applications include bearings - FDA compliant, valve seats, seals.Data provided by Dyneon.
Thermal Conductivity 0.340 - 0.440 W/m-K

@Temperature 100 °C
2.36 - 3.05 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast GOLITE 135 Refractory Insulating Castable
Description: Golite 135 can be used in direct contact with fire and combines a good strength with a high insulation value.Remarks: These values apply to cast products. Also available in gunning vari..
Thermal Conductivity 0.340 - 0.440 W/m-K

@Temperature 1000 °C
2.36 - 3.05 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Gouda Vuurvast GI 26 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Thermal Conductivity 0.340 W/m-K

@Temperature 1370 °C
2.36 BTU-in/hr-ft²-°F

@Temperature 2500 °F
Zircar Ceramics APA-3 Alumina Paper
ZIRCAR Alumina Papers are uniform structures made principally of alumina fiber. APA-3 is a thin uniformly rigidized sheet of alumina fiber and binder. Applications include thermal insulation in lo..
Thermal Conductivity 0.340 - 0.440 W/m-K

@Temperature 600 °C
2.36 - 3.05 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast FI 25-12 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Thermal Conductivity 0.340 - 0.440 W/m-K

@Temperature 200 °C
2.36 - 3.05 BTU-in/hr-ft²-°F

@Temperature 392 °F
Gouda Vuurvast FI 35-12 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.