Material Notes:
Description: Golite 135 can be used in direct contact with fire and combines a good strength with a high insulation value.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 1.35 - 1.45 g/cc
0.0488 - 0.0524 lb/in³
After drying at 110°C
Particle Size <= 3000 µm
<= 3000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 3.00 - 7.00 MPa

@Temperature 1260 °C
435 - 1020 psi

@Temperature 2300 °F
Cold Crushing Strength
8.00 - 12.0 MPa

@Temperature 100 °C
1160 - 1740 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.340 - 0.440 W/m-K

@Temperature 100 °C
2.36 - 3.05 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.370 - 0.470 W/m-K

@Temperature 600 °C
2.57 - 3.26 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.450 - 0.550 W/m-K

@Temperature 1260 °C
3.12 - 3.82 BTU-in/hr-ft²-°F

@Temperature 2300 °F
Maximum Service Temperature, Air 1370 °C
2500 °F
Shrinkage -1.50 - 1.50 %

@Temperature 1260 °C
-1.50 - 1.50 %

@Temperature 2300 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 36 %
36 %
SiO2 44 %
44 %
Descriptive Properties Value Comments
ASTM Classification Q
Material Consumption per 1 m3 1330 kg
Mixing Water 20-25 liters
per 100 kgs dry material