Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.330 W/m-K @Temperature 538 °C |
2.29 BTU-in/hr-ft²-°F @Temperature 1000 °F |
|
Pyrotek Pyrocast AR70 Low-Density Refractory Castable Pyrocast AR70 refractory castable is a high-strength, low-density refractory well suited for specific aluminum foundry applications.ApplicationsSprue Bushings for low pressure die casting Intermedia.. |
|||
Thermal Conductivity | 0.330 W/m-K @Temperature 870 °C |
2.29 BTU-in/hr-ft²-°F @Temperature 1600 °F |
|
Pyrotek NAD-1000 High Temperature Engineering Board NAD-1000 is a high density calcium silicate board reinforced with selected fibers to produce excellent thermal characteristics and dimensional stability up to 1000°C. NAD-1000 retains high strengt.. |
|||
Thermal Conductivity | 0.330 W/m-K @Temperature 1400 °C |
2.29 BTU-in/hr-ft²-°F @Temperature 2550 °F |
|
Zircar Zirconia FBD Zirconia Boards, Discs, and Cylinders Insulation Type FBD Boards, Discs and Cylinders are high strength, uniform, rigid, refractory structures composed of zirconia fibers stabilized with yttria. Type FBD is Zircar Zirconia's strongest and mos.. |
|||
Thermal Conductivity | 0.330 - 0.430 W/m-K @Temperature 1000 °C |
2.29 - 2.98 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Gouda Vuurvast GOLITE LW Refractory Insulating Castable Description: This light weight (LW) castable can be used as a hot face material, as well as for the backlining of a dense castable or brickwork.Remarks: These values apply to cast products. Also ava.. |
|||
Thermal Conductivity | 0.330 - 0.430 W/m-K @Temperature 100 °C |
2.29 - 2.98 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast GOLITE 130 GM Refractory Insulating Castable Description: Golite 130 GM is a standard, medium weight gunning castable, combining a good mechanical strength with a low density and a low thermal conductivity.Remarks: These values apply to cast p.. |
|||
Thermal Conductivity | 0.330 - 0.430 W/m-K @Temperature 100 °C |
2.29 - 2.98 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast GOLITE 130 Refractory Insulating Castable Description: Golite 130 is a standard, medium weight castable, combining a good mechanical strength with a low density and a low thermal conductivity.Remarks: These values apply to cast products. Al.. |
|||
Thermal Conductivity | 0.330 W/m-K @Temperature 800 °C |
2.29 BTU-in/hr-ft²-°F @Temperature 1470 °F |
ASTMÂ C-182 |
Skamol Group VIP 12 Vermiculite Insulating Slab SKAMOL V-1100 & VIP-12 vermiculite slabs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulation of all refractory constr.. |
|||
Thermal Conductivity | 0.330 W/m-K @Temperature 1400 °C |
2.29 BTU-in/hr-ft²-°F @Temperature 2550 °F |
|
Zircar Zirconia FBD Zirconia Boards, Discs, and Cylinders Insulation Type FBD Boards, Discs and Cylinders are high strength, uniform, rigid, refractory structures composed of zirconia fibers stabilized with yttria. Type FBD is Zircar Zirconia's strongest and mos.. |
|||
Thermal Conductivity | 0.330 W/m-K @Temperature 1093 °C |
2.29 BTU-in/hr-ft²-°F @Temperature 1999 °F |
ASTM C182 |
BNZ Materials BNZ-26-60 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.330 W/m-K @Temperature 260 °C |
2.29 BTU-in/hr-ft²-°F @Temperature 500 °F |
ASTM C182 |
BNZ Materials BNZ-28 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.330 W/m-K @Temperature 1000 °C |
2.29 BTU-in/hr-ft²-°F @Temperature 1830 °F |
ASTM C182 |
BNZ Materials BNZP-25L Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |