Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Gouda Vuurvast GOLITE LW Refractory Insulating Castable

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Gouda Vuurvast
Trade Name GOLITE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast GOLITE LW Refractory Insulating Castable.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: This light weight (LW) castable can be used as a hot face material, as well as for the backlining of a dense castable or brickwork.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 1.05 - 1.15 g/cc
0.0379 - 0.0415 lb/in³
After drying at 110°C
Particle Size <= 4000 µm
<= 4000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 1.50 - 2.50 MPa

@Temperature 1000 °C
218 - 363 psi

@Temperature 1830 °F
Cold Crushing Strength
3.50 - 4.50 MPa

@Temperature 100 °C
508 - 653 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.280 - 0.380 W/m-K

@Temperature 100 °C
1.94 - 2.64 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.310 - 0.410 W/m-K

@Temperature 600 °C
2.15 - 2.85 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.330 - 0.430 W/m-K

@Temperature 1000 °C
2.29 - 2.98 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Maximum Service Temperature, Air 1100 °C
2010 °F
Shrinkage -0.600 - 0.200 %

@Temperature 1000 °C
-0.600 - 0.200 %

@Temperature 1830 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 24 %
24 %
SiO2 48 %
48 %
Descriptive Properties Value Comments
Material Consumption per 1 m3 1020 kg
Mixing Water 32-38 liters
per 100 kgs dry material