Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.310 W/m-K @Temperature 600 °C |
2.15 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Pyrotek ISOMAG® 70 Structural Insulation Isomag® 70 is magnesia silicate based formulation provides insulating properties similar to calcium silicate with good strength and dimensional stability up to 1000°C. ApplicationsTorpedo cars La.. |
|||
Thermal Conductivity | 0.310 W/m-K @Temperature 157 °C |
2.15 BTU-in/hr-ft²-°F @Temperature 315 °F |
|
Pyrotek Pyrocast AR LITE Castable Refractory A light weight highly insulating refractory product which offers excellent resistance to molten aluminum erosion and thermal shock.ApplicationsFor conveyance and casting of aluminum and its alloys A.. |
|||
Thermal Conductivity | 0.310 W/m-K @Temperature 204 °C |
2.15 BTU-in/hr-ft²-°F @Temperature 399 °F |
|
Pyrotek NAD-1000 High Temperature Engineering Board NAD-1000 is a high density calcium silicate board reinforced with selected fibers to produce excellent thermal characteristics and dimensional stability up to 1000°C. NAD-1000 retains high strengt.. |
|||
Thermal Conductivity | 0.310 W/m-K @Temperature 1100 °C |
2.15 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Zircar Zirconia FBD Zirconia Boards, Discs, and Cylinders Insulation Type FBD Boards, Discs and Cylinders are high strength, uniform, rigid, refractory structures composed of zirconia fibers stabilized with yttria. Type FBD is Zircar Zirconia's strongest and mos.. |
|||
Thermal Conductivity | 0.310 W/m-K @Temperature 250 °C |
2.15 BTU-in/hr-ft²-°F @Temperature 482 °F |
ASTM E1530 |
3M Dyneon™ CCX1029 PTFE, 10% Carbon Fiber Filled
(discontinued **) Type I, non-free-flowing.Typical Applications: Finished or semi-finished parts: sheets, rods, tubes, billets for skiving of films or machining into complex shapes.Information provided by the Dyneon .. |
|||
Thermal Conductivity | 0.310 W/m-K @Temperature 250 °C |
2.15 BTU-in/hr-ft²-°F @Temperature 482 °F |
ASTM E1530 |
3M Dyneon™ 1750 PTFE Powder
(discontinued **) Type II PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a wide r.. |
|||
Thermal Conductivity | 0.310 W/m-K @Temperature 100 °C |
2.15 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM D1530 |
3M Dyneon™ 1620 PTFE Powder
(discontinued **) Type II, gr. 3 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a.. |
|||
Thermal Conductivity | 0.310 W/m-K @Temperature 100 °C |
2.15 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E1530 |
3M Dyneon™ 1641 PTFE Powder
(discontinued **) Type IV, gr. 2 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a.. |
|||
Thermal Conductivity | 0.310 W/m-K @Temperature 100 °C |
2.15 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E1530 |
3M Dyneon™ 1645 PTFE Powder
(discontinued **) Type IV, gr. 2 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a.. |
|||
Thermal Conductivity | 0.310 - 0.410 W/m-K @Temperature 600 °C |
2.15 - 2.85 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast GOLITE LW Refractory Insulating Castable Description: This light weight (LW) castable can be used as a hot face material, as well as for the backlining of a dense castable or brickwork.Remarks: These values apply to cast products. Also ava.. |
|||
Thermal Conductivity | 0.310 W/m-K @Temperature 800 °C |
2.15 BTU-in/hr-ft²-°F @Temperature 1470 °F |
Parallel to Thickness; ASTM C177-76 |
Zircar Ceramics SALI Alumina Insulation SALI has been serving 1700°C low mass furnace users longer than any other alumina fiber board available today. SALI is a premium grade rigid fiber board with superior hot strength.Information provi.. |
|||
Thermal Conductivity | 0.310 W/m-K @Temperature 200 °C |
2.15 BTU-in/hr-ft²-°F @Temperature 392 °F |
parallel to thickness |
Zircar Refractory Composites ZIRCAL-95 Refractory Board Type ZIRCAL-95 Refractory Board is produced from a combination of natural organic fibers and inert reinforcing fillers in a high density calcium silicate hydrate matrix. Designed as a substitute for.. |
|||
Thermal Conductivity | 0.310 W/m-K @Temperature 1100 °C |
2.15 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Zircar Zirconia FBD Zirconia Boards, Discs, and Cylinders Insulation Type FBD Boards, Discs and Cylinders are high strength, uniform, rigid, refractory structures composed of zirconia fibers stabilized with yttria. Type FBD is Zircar Zirconia's strongest and mos.. |
|||
Thermal Conductivity | 0.310 W/m-K @Temperature 204 °C |
2.15 BTU-in/hr-ft²-°F @Temperature 399 °F |
|
BNZ Materials CS85 High Temperature Structural Insulation NZ manufactures a variety of non-asbestos calcium silicate structural insulations that combine high strength and excellent thermal insulating characteristics for use in a variety of heat processing,.. |