Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.160 W/m-K @Temperature 540 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 1000 °F |
|
Pyrotek Vacuum Formed Shapes for Continuous Sheet Casting Vacuum formed shapes are manufactured from high purity alumina silica fibers in one-piece design that eliminates metal leakage. No pre-heating required. Reusable, with proper treatment, for multip.. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 540 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 1000 °F |
|
Pyrotek Pyrocast L-40 Insulating Refractory Pyrocast L-40 is a fiber free refractory moldable designed for use in contact with molten aluminum. L-40 has excellent workability for use as an insulating lining or patching material.Recommended C.. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 400 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Zircar Zirconia ZYFB-6 Zirconia Boards, Discs, and Cylinders Insulation Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty.. |
|||
Thermal Conductivity | 0.160 - 0.240 W/m-K @Temperature 600 °C |
1.11 - 1.67 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast GOLITE 1.0.6. Mix Refractory Insulating Castable Description: This castable is composed of a high quality alumina cement and vermiculite and is applied as a backlining. Special additives are responsible for the low shrinkage. This castable can be .. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 200 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 392 °F |
Mean temp.; BS 1902 Section 5.5 1991 |
Skamol Group Moler 10 Aggregate Insulation SKAMOL insulating aggregates have the following characteristics: Max. service temperature: Up to 900°C (1652°F)Back-up insulationLightweightGood insulating propertiesChemically inertDue to fre.. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 200 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 392 °F |
Mean temp.; BS 1902 Section 5.5 1991 |
Skamol Group Moler 5 Aggregate Insulation SKAMOL insulating aggregates have the following characteristics: Max. service temperature: Up to 900°C (1652°F)Back-up insulationLightweightGood insulating propertiesChemically inertDue to fre.. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 200 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 392 °F |
Mean temp.; BS 1902 Section 5.5 1991 |
Skamol Group Moler BB-Filler Aggregate Insulation SKAMOL insulating aggregates have the following characteristics: Max. service temperature: Up to 900°C (1652°F)Back-up insulationLightweightGood insulating propertiesChemically inertDue to fre.. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 800 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Zircar Ceramics AL-25/1700 Alumina Insulation AL-25/1700 is a rigid medium duty grade of alumina fiber board. Not as strong as SALI but capable of delivering years of service.Information provided by Zircar Ceramics. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 800 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 1470 °F |
Parallel to thickness; ASTM C177-76 |
Zircar Ceramics AL-30 Alumina Insulation AL-30 and AL-30AA are rigid alumina fiber boards characterized by uniform open porosity and high machinability. Alumina bonded AL-30AA is used in fuel cell reformers.Information provided by Zircar C.. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 800 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 1470 °F |
parallel to thickness; ASTM C177-76 |
Zircar Ceramics AL-30AAH Alumina Insulation AL-30AAH was developed for use in copper vapor lasers where the ultimate in low mass alumina purity is required.Information provided by Zircar Ceramics. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 900 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Zircar Refractory Composites RS-99-45 Refractory Sheet ZRCI Refractory Sheet Type RS-99-45 is comprised of 99% alumina. This "All-Alumina" material is strong, uniform, rigid, refractory structure composed of alpha alumina fibers and high purity inorgani.. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 400 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Zircar Zirconia ZYZ-6 Zirconia Boards and Discs Insulation Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo.. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 649 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Tritex TRI-F Blanket Insulation TRI-F is a unique thermal and acoustic insulation that combines three high temperature fibers in a patented process. The result is a blanket with a service life to 1500°F. By blending fibers of var.. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 1100 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Zircar Refractory Composites ASPA-2 Alumina-Silica Fiber Paper ASPA-2 is a premium grade, lightweight refractory material made from high purity alumina-silica fibers formed into highly flexible sheets. This alumina-silica fiber paper exhibits very low thermal c.. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 1100 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Zircar Refractory Composites ASPA-880 Alumina-Silica Fiber Paper ASPA-880 is a high temperature, lightweight refractory material made from alumina-silica fibers formed into highly flexible sheets. It is made from shorter and smaller diameter fibers with a higher .. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 800 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 1470 °F |
parallel to thickness; ASTM C177 |
Zircar Refractory Composites RS-B ALUMINA-SILICA MOLDABLE ZIRCAR Alumina-Silica Insulating Blanket Type RS-B Moldable is composed of long, high strength ceramic fibers, with an inorganic alumina binder/rigidizing agent. It is a wet blanket that is shipped .. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 538 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 1000 °F |
ASTM C182 |
BNZ Materials BNZ-23A Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 538 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 1000 °F |
ASTM C182 |
BNZ Materials BNZ-24 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 800 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 1470 °F |
Parallel to Thickness; ASTM C177-76 |
Zircar Ceramics AL-30AA Alumina Insulation AL-30 and AL-30AA are rigid alumina fiber boards characterized by uniform open porosity and high machinability. Alumina bonded AL-30AA is used in fuel cell reformers.Information provided by Zircar C.. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 800 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 1470 °F |
Parallel to Thickness |
Zircar Ceramics ASQ Castertip 14 pcf density refractory ceramic fiber "soft tip". Alumina bonding of shot free fiber results in extreme performance in manufacture of the finest grades of medical, food and packaging foils. Inform.. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 1100 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Zircar Refractory Composites ASPA-1 Alumina-Silica Fiber Paper ASPA-1 is a premium grade, lightweight refractory material made from high purity alumina-silica fibers formed into highly flexible sheets. This alumina-silica fiber paper exhibits very low thermal c.. |
|||
Thermal Conductivity | 0.160 W/m-K @Temperature 400 °C |
1.11 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Zircar Zirconia ZYZ-6 Zirconia Boards and Discs Insulation Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo.. |